Effect of sintering holding time on the properties and low-temperature degradation behaviour of manganese oxide-doped Y-TZP ceramic
The sintering of yttria-tetragonal zirconia polycrystals (Y-TZP) is commonly carried at a predefined temperature using a long holding time of 2 hours. This often has resulted in grain coarsening which affects the mechanical properties of the sintered body and low temperature degradation (LTD) behavi...