Influence of Eu3+ Ions on Elastic Moduli and Microhardness of Zinc‑boro‑soda‑lime‑silica Glass System

This study focuses on zinc-boro-soda-lime-silica (ZnO− B2O3−SLS) glasses produced through fast-cooling melt-quenching. The influence of Eu3+ ions on glass properties is explored. As Eu3+ concentration rises, bulk density and molar volume increase from 3.423 to 3.484 g/cm3 and 21.760 to 23.768 cm3 /...

Full description

Saved in:
Bibliographic Details
Main Authors: Cheong, Wei Mun, Mohd Zaid, Mohd Hafz, Matori, Khamirul Amin, Fen, Yap Wing, Tee, Tan Sin, Loh, Zhi Wei, Mayzan, Mohd Zul Hilmi
Format: Article
Language:English
Published: Springer 2024
Subjects:
Online Access:http://eprints.uthm.edu.my/11872/1/J17487_cf5dc51a197323ac78e75260497cd52c.pdf
http://eprints.uthm.edu.my/11872/
https://doi.org/10.1007/s12633-024-02918-9
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universiti Tun Hussein Onn Malaysia
Language: English
Description
Summary:This study focuses on zinc-boro-soda-lime-silica (ZnO− B2O3−SLS) glasses produced through fast-cooling melt-quenching. The influence of Eu3+ ions on glass properties is explored. As Eu3+ concentration rises, bulk density and molar volume increase from 3.423 to 3.484 g/cm3 and 21.760 to 23.768 cm3 /mol, respectively. X-ray diffraction indicates amorphous phase dominance supported by glassy surface morphology. Ultrasonic measurements show the increasing and decreasing trend for ultrasonic velocities and elastic moduli with increasing Eu3+ concentration. Poisson’s ratio of the samples signifes their low cross-link density behavior. Moreover, the ZBS-3Eu presents the highest microhardness value of 4.776 GPa. The sample’s fractal bond connectivity varies from 1.814 to 2.051, suggesting a 2D structure. Likewise, the ZBS-3Eu glass sample exhibits the most rigidity attributed to its highest fg value of 0.075. These findings suggest that ZBS-3Eu has the potential for applications requiring high-strength glass.