Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading
The use of catalyst in the biomass gasification is effective to elevate hydrogen content and to reduce tar formation. This study presents the development of 2.5-10 wt% Fe/CeO2 catalysts for biomass gasification to hydrogen. The catalysts were prepared using incipient wetness impregnation method....
Saved in:
Main Authors: | , , |
---|---|
Format: | Book Section |
Published: |
American Institute of Physics
2012
|
Subjects: | |
Online Access: | http://eprints.utp.edu.my/8666/1/AIP-MasFatiha%26Anita-ICONT2011.pdf http://eprints.utp.edu.my/8666/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Teknologi Petronas |
id |
my.utp.eprints.8666 |
---|---|
record_format |
eprints |
spelling |
my.utp.eprints.86662017-01-19T08:22:01Z Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading Mohamad, Mas Fatiha Ramli, Anita Yusup, Suzana TP Chemical technology QD Chemistry The use of catalyst in the biomass gasification is effective to elevate hydrogen content and to reduce tar formation. This study presents the development of 2.5-10 wt% Fe/CeO2 catalysts for biomass gasification to hydrogen. The catalysts were prepared using incipient wetness impregnation method. Different characterization methods such as Powder X-Ray Diffraction (XRD), Temperature Programmed Reduction(TPR), N2 adsorption-desorption isotherm and Field Emission Scanning Electron Microscopy (FESEM) were used to characterize the prepared catalysts. BET analysis clearly indicates that Fe/CeO2 catalysts are mainly nonporous and the surface area of the catalysts increases with increasing of Fe loading. Characterization by XRD exhibited the formation of a solid solution of iron-cerium oxide, with the presence of cubic CeO2 structure which is in agreement with FESEM images. The TPR results show the emergence of two reduction peaks, corresponding to the surface and bulk reduction of CeO2 to Ce2O3. No distinct peak related to the reduction of Fe2O3 to Fe3O4, instead a shoulder evolved, related to the reduction of Fe3O4 to Fe. American Institute of Physics 2012 Book Section PeerReviewed application/pdf http://eprints.utp.edu.my/8666/1/AIP-MasFatiha%26Anita-ICONT2011.pdf Mohamad, Mas Fatiha and Ramli, Anita and Yusup, Suzana (2012) Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading. In: International Conference on Nanotechnology - Research and Commercialization 2011. American Institute of Physics, pp. 288-297. http://eprints.utp.edu.my/8666/ |
institution |
Universiti Teknologi Petronas |
building |
UTP Resource Centre |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Teknologi Petronas |
content_source |
UTP Institutional Repository |
url_provider |
http://eprints.utp.edu.my/ |
topic |
TP Chemical technology QD Chemistry |
spellingShingle |
TP Chemical technology QD Chemistry Mohamad, Mas Fatiha Ramli, Anita Yusup, Suzana Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading |
description |
The use of catalyst in the biomass gasification is effective to elevate hydrogen content and to reduce tar
formation. This study presents the development of 2.5-10 wt%
Fe/CeO2 catalysts for biomass gasification to hydrogen. The
catalysts were prepared using incipient wetness impregnation
method. Different characterization methods such as Powder X-Ray Diffraction (XRD), Temperature Programmed Reduction(TPR), N2 adsorption-desorption isotherm and Field Emission
Scanning Electron Microscopy (FESEM) were used to characterize the prepared catalysts. BET analysis clearly
indicates that Fe/CeO2 catalysts are mainly nonporous and the surface area of the catalysts increases with increasing of Fe loading. Characterization by XRD exhibited the formation of a solid solution of iron-cerium oxide, with the presence of cubic CeO2 structure which is in agreement with FESEM images. The TPR results show the emergence of two reduction peaks, corresponding to the surface and bulk reduction of CeO2 to Ce2O3. No distinct peak related to the reduction of Fe2O3 to Fe3O4, instead a shoulder evolved, related to the reduction of Fe3O4 to Fe. |
format |
Book Section |
author |
Mohamad, Mas Fatiha Ramli, Anita Yusup, Suzana |
author_facet |
Mohamad, Mas Fatiha Ramli, Anita Yusup, Suzana |
author_sort |
Mohamad, Mas Fatiha |
title |
Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading |
title_short |
Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading |
title_full |
Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading |
title_fullStr |
Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading |
title_full_unstemmed |
Study on the physicochemical properties of Fe/CeO2 catalysts as an effect from different iron loading |
title_sort |
study on the physicochemical properties of fe/ceo2 catalysts as an effect from different iron loading |
publisher |
American Institute of Physics |
publishDate |
2012 |
url |
http://eprints.utp.edu.my/8666/1/AIP-MasFatiha%26Anita-ICONT2011.pdf http://eprints.utp.edu.my/8666/ |
_version_ |
1738655672579391488 |