Photocatalytic activity of La-doped ZnO nanostructure materials synthesized by sonochemical method
© 2015, The Nonferrous Metals Society of China and Springer-Verlag Berlin Heidelberg. ZnO nanostructure materials doped with different La contents were synthesized by sonochemical method. The products were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission ele...
محفوظ في:
المؤلفون الرئيسيون: | , , , , , |
---|---|
التنسيق: | دورية |
منشور في: |
2017
|
الوصول للمادة أونلاين: | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84931364104&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/41904 |
الوسوم: |
إضافة وسم
لا توجد وسوم, كن أول من يضع وسما على هذه التسجيلة!
|
الملخص: | © 2015, The Nonferrous Metals Society of China and Springer-Verlag Berlin Heidelberg. ZnO nanostructure materials doped with different La contents were synthesized by sonochemical method. The products were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), Raman spectroscopy, and Fourier transform infrared spectroscopy (FTIR). In this research, XRD patterns of pure ZnO and La-doped ZnO are specified as hexagonal wurtzite ZnO structure with no detection of La 2 O 3 phase. SEM and TEM characterization revealed the flower shape of pure ZnO built-up from petals of hexagonal prisms with hexagonal pyramid tips. Upon doping with La, the flower-shaped ZnO is broken into individual 1D prism-like nanorods. Photocatalytic activities of the as-synthesized products were determined by measuring the degradation of methylene blue (MB) under ultraviolet–visible (UV) light irradiation. Among them, the 2.0 mol% La-doped ZnO shows better photocatalytic properties than any other products. |
---|