Piezoelectric properties of Pb0.985Sr0.01[(Zn 1/3Nb2/3)xTiyZrz]O 3 ceramics doped with 0.05 mol% Sb2O5
Ceramic solid solutions within the system Pb0.985Sr0.01[(Zn1/3Nb2/3)xTiyZrz]O3doped with 0.05 mol% Sb2O5, where x = 0.02, 0.04, 0.06, 0.08 and 0.10, y = 0.46, 0.45, 0.44, 0.43 and 0.42 and z = 0.52, 0.51, 0.50, 0.49 and 0.48, were prepared by solid state reaction. The phase formation, microstructure...
Saved in:
Main Authors: | , |
---|---|
格式: | Conference Proceeding |
出版: |
2018
|
主題: | |
在線閱讀: | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=70450029598&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/49443 |
標簽: |
添加標簽
沒有標簽, 成為第一個標記此記錄!
|
總結: | Ceramic solid solutions within the system Pb0.985Sr0.01[(Zn1/3Nb2/3)xTiyZrz]O3doped with 0.05 mol% Sb2O5, where x = 0.02, 0.04, 0.06, 0.08 and 0.10, y = 0.46, 0.45, 0.44, 0.43 and 0.42 and z = 0.52, 0.51, 0.50, 0.49 and 0.48, were prepared by solid state reaction. The phase formation, microstructure, dielectric properties and piezoelectric properties of this system were investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM) and electrical measurements. All compositions exhibit complete solid solutions of pure perovskite phases. The dielectric properties decrease with increasing content of the B1sites (Zn1/3Nb2/3)x. The maximum dielectric constant is about 25000. This observation suggests that the B-site substitution directly affects the dielectric properties, d33 constants and remanent polarization of this ceramic system. © 2009 American Institute of Physics. |
---|