Surface modification of γ-TiAl alloys by acetylene plasma deposition
Surfaces of two γ-TiAl alloys, Ti-47 at% Al-2at% Nb-2 at% Cr (MJ12) and Ti-47 at% Al-2 at% Nb-2 at% Mn + 0.8 at% TiB2 (MJ47), have been modified by acetylene plasma deposition at bias voltages of -4, -5 and -6 kV for 3.6 × 103 s (1 h) and 1.44 × 104 s (4 h). Knoop hardness (HK) of the alloys is incr...
Saved in:
Main Authors: | Narksitipan S., Thongtem T., McNallan M., Thongtem S. |
---|---|
Format: | Article |
Language: | English |
Published: |
2014
|
Online Access: | http://www.scopus.com/inward/record.url?eid=2-s2.0-33748980224&partnerID=40&md5=fe49369192b4b2b23e66e3ef25f35812 http://cmuir.cmu.ac.th/handle/6653943832/5066 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Chiang Mai University |
Language: | English |
Similar Items
-
Surface modification of γ-TiAl alloys by acetylene plasma deposition
by: Suparut Narksitipan, et al.
Published: (2018) -
Acetylene plasma deposition on gamma-TiAl alloys
by: Narksitipan S., et al.
Published: (2014) -
Acetylene plasma deposition on gamma-TiAl alloys
by: S. Narksitipan, et al.
Published: (2018) -
Surface modification of the γ-TiAl alloys by the nitridation
by: Sopunna K., et al.
Published: (2014) -
Deposition of TiC on γ-TiAl alloys by directly applying voltages
by: Boonruang C., et al.
Published: (2014)