Pisitpipathsin, N., Pengpat, K., Eitssayeam, S., Tunkasiri, T., Sirisoonthorn, S., Budchan, S., & Intatha, U. (2018). Low sintering temperature of lead magnesium niobate-lead titanate (0.9PMN-0.1PT) by adding oxide additives.
استشهاد بنمط شيكاغوPisitpipathsin, Nuttapon, Kamonpan Pengpat, Sukum Eitssayeam, Tawee Tunkasiri, Somnuk Sirisoonthorn, Savittree Budchan, و Uraiwan Intatha. Low Sintering Temperature of Lead Magnesium Niobate-lead Titanate (0.9PMN-0.1PT) By Adding Oxide Additives. 2018.
MLA استشهادPisitpipathsin, Nuttapon, et al. Low Sintering Temperature of Lead Magnesium Niobate-lead Titanate (0.9PMN-0.1PT) By Adding Oxide Additives. 2018.