Glycolthermal synthesis and characterization of hexagonal CdS round microparticles in flower-like clusters

Hexagonal CdS round microparticles in flower-like clusters were synthesized by glycolthermal reactions of CdCl2 and thiourea as cadmium and sulphur sources in 1,2-propylene glycol (PG) at 100-200 °C for 10-30 h. Phase and morphology were detected using X-ray diffraction (XRD), and scanning and trans...

全面介紹

Saved in:
書目詳細資料
Main Authors: Phuruangrat A., Ekthammathat N., Thongtem T., Thongtem S.
格式: Article
語言:English
出版: 2014
在線閱讀:http://www.scopus.com/inward/record.url?eid=2-s2.0-80052969751&partnerID=40&md5=3985bead41b932e85ef6520363300067
http://cmuir.cmu.ac.th/handle/6653943832/6442
標簽: 添加標簽
沒有標簽, 成為第一個標記此記錄!
機構: Chiang Mai University
語言: English
實物特徵
總結:Hexagonal CdS round microparticles in flower-like clusters were synthesized by glycolthermal reactions of CdCl2 and thiourea as cadmium and sulphur sources in 1,2-propylene glycol (PG) at 100-200 °C for 10-30 h. Phase and morphology were detected using X-ray diffraction (XRD), and scanning and transmission electron microscopy (SEM, TEM). The products were pure phase of hexagonal wurtzite CdS. The quantitative elemental analysis of Cd:S ratio was detected using energy dispersive X-ray (EDX) analyzer. Raman spectrometer revealed the presence of fundamental and overtone modes at 296 and 595 cm -1, corresponding to the strong 1LO and weak 2LO modes, respectively. Photonic properties were investigated using UV-visible and photoluminescence (PL) spectroscopy. They showed the same absorption at 493-498 nm, and emission at 431 nm due to the excitonic recombination process. A possible formation mechanism was also proposed, according to experimental results. © 2011 Elsevier B.V.