Dielectric, ferroelectric and piezoelectric properties of 0-3 barium titanate-Portland cement composites
In this work, barium titanate (BT) and cement composites of 0-3 connectivity were produced with BT concentrations of 30%, 50% and 70% by volume using the mixing and pressing method. The dielectric constant (εr ) and the dielectric loss (tan δ) at room temperature and at various frequencies (0.1-20 k...