Photoemission and energy gap of MgWO 4 particles connecting as nanofibers synthesized by electrospinning-calcination combinations

Mixtures of magnesium acetate tetrahydrate ((CH 3COO) 2Mg·4H 2O), ammonium tungstate tetrahydrate ((NH 4) 6W 7O 24·4H 2O), and poly(vinyl alcohol) with the molecular weight of 72,000 were electrospun through a +15 kV direct voltage to form fibers on ground flat aluminum foils. The electrospun fibers...

全面介紹

Saved in:
書目詳細資料
Main Authors: Wannapop S., Thongtem T., Thongtem S.
格式: Article
語言:English
出版: 2014
在線閱讀:http://www.scopus.com/inward/record.url?eid=2-s2.0-84857786739&partnerID=40&md5=8f6e68a1164250bf8fd756afa9c92cc9
http://cmuir.cmu.ac.th/handle/6653943832/6826
標簽: 添加標簽
沒有標簽, 成為第一個標記此記錄!
機構: Chiang Mai University
語言: English
實物特徵
總結:Mixtures of magnesium acetate tetrahydrate ((CH 3COO) 2Mg·4H 2O), ammonium tungstate tetrahydrate ((NH 4) 6W 7O 24·4H 2O), and poly(vinyl alcohol) with the molecular weight of 72,000 were electrospun through a +15 kV direct voltage to form fibers on ground flat aluminum foils. The electrospun fibers of 1.5, 3.0, and 4.5 mmol of each starting material containing 1.3 g poly(vinyl alcohol) were further calcined at 500-700 °C for 3 h constant length of time. At 500 and 600 °C calcination, both monoclinic and anorthic phases of MgWO 4 particles with different sizes connecting as fibrous assemblies were detected. Upon increasing the calcination temperature to 700 °C, only monoclinic phase of facet nanoparticles interconnecting along the fibrous axes with 4.19 eV indirect band gap and 461 nm photoemission was synthesized. In the present research, formation of MgWO 4 molecules as well as nucleation and growth of nanoparticles was also proposed. © 2012 Elsevier B.V. All rights reserved.