Magnetite Core-Cadmium Imprinted Poly(Aniline-Formaldehyde) for Cd(II) Preconcentration and Analysis

<p align="justify">Cadmium determination in environmental samples are interesting because of its high toxicity. Atomic Absorption Spectroscopy (AAS) can be used to measure cadmium concentration, unfortunately the sensitivity is low in trace concentration so preconcetration step is ne...

Full description

Saved in:
Bibliographic Details
Main Author: IRHAM FAUZI ABSHAR (NIM: 10512051)
Format: Final Project
Language:Indonesia
Online Access:https://digilib.itb.ac.id/gdl/view/28126
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Institut Teknologi Bandung
Language: Indonesia
id id-itb.:28126
spelling id-itb.:281262018-10-11T13:01:24ZMagnetite Core-Cadmium Imprinted Poly(Aniline-Formaldehyde) for Cd(II) Preconcentration and Analysis IRHAM FAUZI ABSHAR (NIM: 10512051), Indonesia Final Project INSTITUT TEKNOLOGI BANDUNG https://digilib.itb.ac.id/gdl/view/28126 <p align="justify">Cadmium determination in environmental samples are interesting because of its high toxicity. Atomic Absorption Spectroscopy (AAS) can be used to measure cadmium concentration, unfortunately the sensitivity is low in trace concentration so preconcetration step is needed. Magnetite core-cadmium imprinted poly(aniline-formaldehyde) (Fe3O4@Cd-IPAF) was successfully synthetized for selective adsorption and preconcentration of Cd(II). SEM images from magnetite (Fe3O4) and Fe3O4@Cd-IPAF showed that magnetite was successfully coated by IIP and the result of Energy Dispersive X-Ray Spectrometry (EDS) characterization proved that there was amount of cadmium from the material. Retention characterization using batch method showed that the optimal contidion of Fe3O4@Cd-IPAF was at pH 6, 32 minutes of contact time with recovery percentage 106,6%. Adsorption capacity of NIP (non imprinted polymer) and IIP (ion imprinted polymer) were found to be 2,66mg/g and 4,33mg/g. The selectivity coefficient for binary mixtures of Cd2+/Cu2+, Cd2+/Pb2+ and Cd2+/Ni2+ was 1,33; 1,67 and 11,2 respectively. Magnetite core-cadmium imprinted poly(aniline-formaldehyde) was selective because of the selectivity coefficients are greater than 1. After preconcentration, the sensitivity of FAAS methods increased 6520 times. Analysis and preconcentration of river water using Fe3O4@Cd-IPAF shown the concentration of cadmium was 19 ppb.<p align="justify"> text
institution Institut Teknologi Bandung
building Institut Teknologi Bandung Library
continent Asia
country Indonesia
Indonesia
content_provider Institut Teknologi Bandung
collection Digital ITB
language Indonesia
description <p align="justify">Cadmium determination in environmental samples are interesting because of its high toxicity. Atomic Absorption Spectroscopy (AAS) can be used to measure cadmium concentration, unfortunately the sensitivity is low in trace concentration so preconcetration step is needed. Magnetite core-cadmium imprinted poly(aniline-formaldehyde) (Fe3O4@Cd-IPAF) was successfully synthetized for selective adsorption and preconcentration of Cd(II). SEM images from magnetite (Fe3O4) and Fe3O4@Cd-IPAF showed that magnetite was successfully coated by IIP and the result of Energy Dispersive X-Ray Spectrometry (EDS) characterization proved that there was amount of cadmium from the material. Retention characterization using batch method showed that the optimal contidion of Fe3O4@Cd-IPAF was at pH 6, 32 minutes of contact time with recovery percentage 106,6%. Adsorption capacity of NIP (non imprinted polymer) and IIP (ion imprinted polymer) were found to be 2,66mg/g and 4,33mg/g. The selectivity coefficient for binary mixtures of Cd2+/Cu2+, Cd2+/Pb2+ and Cd2+/Ni2+ was 1,33; 1,67 and 11,2 respectively. Magnetite core-cadmium imprinted poly(aniline-formaldehyde) was selective because of the selectivity coefficients are greater than 1. After preconcentration, the sensitivity of FAAS methods increased 6520 times. Analysis and preconcentration of river water using Fe3O4@Cd-IPAF shown the concentration of cadmium was 19 ppb.<p align="justify">
format Final Project
author IRHAM FAUZI ABSHAR (NIM: 10512051),
spellingShingle IRHAM FAUZI ABSHAR (NIM: 10512051),
Magnetite Core-Cadmium Imprinted Poly(Aniline-Formaldehyde) for Cd(II) Preconcentration and Analysis
author_facet IRHAM FAUZI ABSHAR (NIM: 10512051),
author_sort IRHAM FAUZI ABSHAR (NIM: 10512051),
title Magnetite Core-Cadmium Imprinted Poly(Aniline-Formaldehyde) for Cd(II) Preconcentration and Analysis
title_short Magnetite Core-Cadmium Imprinted Poly(Aniline-Formaldehyde) for Cd(II) Preconcentration and Analysis
title_full Magnetite Core-Cadmium Imprinted Poly(Aniline-Formaldehyde) for Cd(II) Preconcentration and Analysis
title_fullStr Magnetite Core-Cadmium Imprinted Poly(Aniline-Formaldehyde) for Cd(II) Preconcentration and Analysis
title_full_unstemmed Magnetite Core-Cadmium Imprinted Poly(Aniline-Formaldehyde) for Cd(II) Preconcentration and Analysis
title_sort magnetite core-cadmium imprinted poly(aniline-formaldehyde) for cd(ii) preconcentration and analysis
url https://digilib.itb.ac.id/gdl/view/28126
_version_ 1822021596890529792