RESULT ANALYSIS OF FRICTION STIR WELDING OF ALUMINUM 5083 H112 USING TRIANGULAR PIN TOOL WITH VARIATION IN ROTATIONAL AND TRANSLATION SPEED

Needs of aluminium as material for the manufacture of transportation vehicle is very large in Indonesia. Joint process such as welding is needed for producing large-sized transportation vehicle. Friction stir welding is a type of welding without melting the workpiece. The welding is done by the pres...

Full description

Saved in:
Bibliographic Details
Main Author: Yazid, Muhammad
Format: Final Project
Language:Indonesia
Online Access:https://digilib.itb.ac.id/gdl/view/53044
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Institut Teknologi Bandung
Language: Indonesia
id id-itb.:53044
spelling id-itb.:530442021-02-26T18:59:23ZRESULT ANALYSIS OF FRICTION STIR WELDING OF ALUMINUM 5083 H112 USING TRIANGULAR PIN TOOL WITH VARIATION IN ROTATIONAL AND TRANSLATION SPEED Yazid, Muhammad Indonesia Final Project Friction stir welding, aluminium 5083 H112, welding parameter INSTITUT TEKNOLOGI BANDUNG https://digilib.itb.ac.id/gdl/view/53044 Needs of aluminium as material for the manufacture of transportation vehicle is very large in Indonesia. Joint process such as welding is needed for producing large-sized transportation vehicle. Friction stir welding is a type of welding without melting the workpiece. The welding is done by the presence of friction between the tool and the workpiece. This research was conducted to determine the effect of rotation and translation speed on the quality of welding result in 10 mm-Aluminium 5083 H112. The tool used is AISI H13 Steel with a threaded triangular pin shape. This pin has a triangle length of 9 mm and a pin length of 9.5 mm. The type of thread used is the right thread. The results of optimization process produce parameter variatons on translation speed and dwell treatment. The varied translation speeds were 50 mm/min and 75 mm/min at a rotation speed 1500 rpm. The weld areas such as weld nugget (WN), heat affected zone (HAZ), and thermomechanically affected zone (TMAZ) have been changed in microstructure caused by the process of welding. Differences in parameters will cause in the size of formed defect. The value of joint strength, hardness, and toughness have increased with an increase in translation speed. The best welding result are produced by welding parameter with translation speed 75 mm/min. text
institution Institut Teknologi Bandung
building Institut Teknologi Bandung Library
continent Asia
country Indonesia
Indonesia
content_provider Institut Teknologi Bandung
collection Digital ITB
language Indonesia
description Needs of aluminium as material for the manufacture of transportation vehicle is very large in Indonesia. Joint process such as welding is needed for producing large-sized transportation vehicle. Friction stir welding is a type of welding without melting the workpiece. The welding is done by the presence of friction between the tool and the workpiece. This research was conducted to determine the effect of rotation and translation speed on the quality of welding result in 10 mm-Aluminium 5083 H112. The tool used is AISI H13 Steel with a threaded triangular pin shape. This pin has a triangle length of 9 mm and a pin length of 9.5 mm. The type of thread used is the right thread. The results of optimization process produce parameter variatons on translation speed and dwell treatment. The varied translation speeds were 50 mm/min and 75 mm/min at a rotation speed 1500 rpm. The weld areas such as weld nugget (WN), heat affected zone (HAZ), and thermomechanically affected zone (TMAZ) have been changed in microstructure caused by the process of welding. Differences in parameters will cause in the size of formed defect. The value of joint strength, hardness, and toughness have increased with an increase in translation speed. The best welding result are produced by welding parameter with translation speed 75 mm/min.
format Final Project
author Yazid, Muhammad
spellingShingle Yazid, Muhammad
RESULT ANALYSIS OF FRICTION STIR WELDING OF ALUMINUM 5083 H112 USING TRIANGULAR PIN TOOL WITH VARIATION IN ROTATIONAL AND TRANSLATION SPEED
author_facet Yazid, Muhammad
author_sort Yazid, Muhammad
title RESULT ANALYSIS OF FRICTION STIR WELDING OF ALUMINUM 5083 H112 USING TRIANGULAR PIN TOOL WITH VARIATION IN ROTATIONAL AND TRANSLATION SPEED
title_short RESULT ANALYSIS OF FRICTION STIR WELDING OF ALUMINUM 5083 H112 USING TRIANGULAR PIN TOOL WITH VARIATION IN ROTATIONAL AND TRANSLATION SPEED
title_full RESULT ANALYSIS OF FRICTION STIR WELDING OF ALUMINUM 5083 H112 USING TRIANGULAR PIN TOOL WITH VARIATION IN ROTATIONAL AND TRANSLATION SPEED
title_fullStr RESULT ANALYSIS OF FRICTION STIR WELDING OF ALUMINUM 5083 H112 USING TRIANGULAR PIN TOOL WITH VARIATION IN ROTATIONAL AND TRANSLATION SPEED
title_full_unstemmed RESULT ANALYSIS OF FRICTION STIR WELDING OF ALUMINUM 5083 H112 USING TRIANGULAR PIN TOOL WITH VARIATION IN ROTATIONAL AND TRANSLATION SPEED
title_sort result analysis of friction stir welding of aluminum 5083 h112 using triangular pin tool with variation in rotational and translation speed
url https://digilib.itb.ac.id/gdl/view/53044
_version_ 1822929213446946816