THE EFFECT OF H3BO3 AND B2O3 ADDITION ON NICKEL MATTE FORMATION FROM SAPROLITIC NICKEL ORE AT 1100ºC-1350ºC
Saprolite nickel laterite ores are generally processed to produce ferronickel containing 10-30% Ni and 70-90% Fe, which can be used for manufacturing of stainless steel and other alloys. Commonly used technology for processing laterite nickel ore through pyrometallurgical routes is the Rotary Kil...
Saved in:
Main Author: | Miertha Nadya Salsabilla, Ayu |
---|---|
Format: | Theses |
Language: | Indonesia |
Online Access: | https://digilib.itb.ac.id/gdl/view/57909 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Institut Teknologi Bandung |
Language: | Indonesia |
Similar Items
-
NITRIFICATION RATE OF SEAWATER SUBMERGED BIOFILTER AT THREE DIFFERENT OPERATING TEMPERATURES (15ºC, 25ºC DAN 35º CC)
by: Lestari Taufan, Winda -
ALTERNATIVE SOURCES OF SULPHUR TO PRODUCE NICKEL MATTE FROM SAPROLITE TYPE NICKEL LATERITES ORE
by: Miertha Nadya Salsabilla, Ayu -
STUDY OF FERRONICKEL FORMATION FROM NICKEL SAPROLITE ORE AT 900-1300 ̼̉C BY COAL AND ADDITION OF CaCl2 AND CaO
by: MUKTI PRASOJO (NIM : 12514036), RACHMAT -
STUDY OF EFFECT OF CaSO4 AND H3BO3 ADDITION ON NICKEL MATTE PARTICLE FORMATION USING SAPROLITIC NICKEL ORE AT 1100?C-1300?C
by: Satria Putra, Irfan -
ISOTHERMAL OXIDATION BEHAVIOUR STUDY OF AL0.5COCRCUFENI HIGH ENTROPY ALLOY AT 800, 900, AND 1000ºC
by: Maulana Ma'ruf, Zaid