Background. Many studies use immersion in liquid substances within different as a method to measure various physical and mechanical properties of dental materials. However, these conditions differ when saliva or other liquid materials were in the human oral cavity. Saliva flow was certainly out peri...

Full description

Saved in:
Bibliographic Details
Main Author: Imam Safari Azhar
Format: Theses and Dissertations NonPeerReviewed
Language:Indonesian
Published: 2010
Subjects:
Online Access:https://repository.unair.ac.id/118253/1/KKA%20KK%20KG%2070-11%20Azh%20p.pdf
https://repository.unair.ac.id/118253/
http://www.lib.unair.ac.id
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universitas Airlangga
Language: Indonesian
id id-langga.118253
record_format dspace
spelling id-langga.1182532022-10-20T02:43:12Z https://repository.unair.ac.id/118253/ Perbedaan Antara Kelarutan Komposit Hybrid Setelah Penetesan Dan Perenaman Saliva Buatan pH4 (Ekperimental Laboratorik) Imam Safari Azhar R Medicine RK1-715 Dentistry Background. Many studies use immersion in liquid substances within different as a method to measure various physical and mechanical properties of dental materials. However, these conditions differ when saliva or other liquid materials were in the human oral cavity. Saliva flow was certainly out periodically through the duct indirect teeth submerged in saliva. . Then came the idea to use a more appropriate method of hatching the physiological state of the oral cavity. droplets use hybrid composites with liquid acid. Acid caused degradation / damage to the surface of composite resins. So the researcher wanted to know the differences between solubility hybrid type composite restorative materials on the hatching and artificial saliva immersion pH 4 as a preliminary study to be developed for the advancement of science.Purpose. The aim of this study was to know the difference between the solubility in hybrid composite type in droplets with pH 4 artificial saliva and pH 4 artificial saliva immersion. Method. the method of this study was experimental laboratories research. About 14 samples of composite was formed with 5mm diameters and 3mm thickness. Group 1, samples was immersed in artificial saliva with pH 4 for one week. Group 2, samples was dropped in artificial saliva with pH 4 for one week. All samples of each groups were examined by reducing the final weight afier treatment minus initial weight. Result. There was significant differences between the drops of pH 4 artificial saliva and the immersion of pH 4 artificial saliva on hybrid composite solubility. Conclusion. The saliva droplets in composit hybrid showed more great solubility than saliva immersion. 2010 Thesis NonPeerReviewed text id https://repository.unair.ac.id/118253/1/KKA%20KK%20KG%2070-11%20Azh%20p.pdf Imam Safari Azhar (2010) Perbedaan Antara Kelarutan Komposit Hybrid Setelah Penetesan Dan Perenaman Saliva Buatan pH4 (Ekperimental Laboratorik). Skripsi thesis, UNIVERSITAS AIRLANGGA. http://www.lib.unair.ac.id
institution Universitas Airlangga
building Universitas Airlangga Library
continent Asia
country Indonesia
Indonesia
content_provider Universitas Airlangga Library
collection UNAIR Repository
language Indonesian
topic R Medicine
RK1-715 Dentistry
spellingShingle R Medicine
RK1-715 Dentistry
Imam Safari Azhar
Perbedaan Antara Kelarutan Komposit Hybrid Setelah Penetesan Dan Perenaman Saliva Buatan pH4 (Ekperimental Laboratorik)
description Background. Many studies use immersion in liquid substances within different as a method to measure various physical and mechanical properties of dental materials. However, these conditions differ when saliva or other liquid materials were in the human oral cavity. Saliva flow was certainly out periodically through the duct indirect teeth submerged in saliva. . Then came the idea to use a more appropriate method of hatching the physiological state of the oral cavity. droplets use hybrid composites with liquid acid. Acid caused degradation / damage to the surface of composite resins. So the researcher wanted to know the differences between solubility hybrid type composite restorative materials on the hatching and artificial saliva immersion pH 4 as a preliminary study to be developed for the advancement of science.Purpose. The aim of this study was to know the difference between the solubility in hybrid composite type in droplets with pH 4 artificial saliva and pH 4 artificial saliva immersion. Method. the method of this study was experimental laboratories research. About 14 samples of composite was formed with 5mm diameters and 3mm thickness. Group 1, samples was immersed in artificial saliva with pH 4 for one week. Group 2, samples was dropped in artificial saliva with pH 4 for one week. All samples of each groups were examined by reducing the final weight afier treatment minus initial weight. Result. There was significant differences between the drops of pH 4 artificial saliva and the immersion of pH 4 artificial saliva on hybrid composite solubility. Conclusion. The saliva droplets in composit hybrid showed more great solubility than saliva immersion.
format Theses and Dissertations
NonPeerReviewed
author Imam Safari Azhar
author_facet Imam Safari Azhar
author_sort Imam Safari Azhar
title Perbedaan Antara Kelarutan Komposit Hybrid Setelah Penetesan Dan Perenaman Saliva Buatan pH4 (Ekperimental Laboratorik)
title_short Perbedaan Antara Kelarutan Komposit Hybrid Setelah Penetesan Dan Perenaman Saliva Buatan pH4 (Ekperimental Laboratorik)
title_full Perbedaan Antara Kelarutan Komposit Hybrid Setelah Penetesan Dan Perenaman Saliva Buatan pH4 (Ekperimental Laboratorik)
title_fullStr Perbedaan Antara Kelarutan Komposit Hybrid Setelah Penetesan Dan Perenaman Saliva Buatan pH4 (Ekperimental Laboratorik)
title_full_unstemmed Perbedaan Antara Kelarutan Komposit Hybrid Setelah Penetesan Dan Perenaman Saliva Buatan pH4 (Ekperimental Laboratorik)
title_sort perbedaan antara kelarutan komposit hybrid setelah penetesan dan perenaman saliva buatan ph4 (ekperimental laboratorik)
publishDate 2010
url https://repository.unair.ac.id/118253/1/KKA%20KK%20KG%2070-11%20Azh%20p.pdf
https://repository.unair.ac.id/118253/
http://www.lib.unair.ac.id
_version_ 1748192803674914816