Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties

It has been studied in this work the change of physical and chemical properties of Fe203-pillared clay. The pillared clay has been synthesized by intercalating polyoxycation of the iron into the interlayer of the montmorillortite clay. The intercalated compound then was calcinated at various tempera...

Full description

Saved in:
Bibliographic Details
Main Author: Perpustakaan UGM, i-lib
Format: Article NonPeerReviewed
Published: [Yogyakarta] : Universitas Gadjah Mada 2004
Subjects:
Online Access:https://repository.ugm.ac.id/17641/
http://i-lib.ugm.ac.id/jurnal/download.php?dataId=402
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universitas Gadjah Mada
id id-ugm-repo.17641
record_format dspace
spelling id-ugm-repo.176412014-06-18T00:29:16Z https://repository.ugm.ac.id/17641/ Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties Perpustakaan UGM, i-lib Jurnal i-lib UGM It has been studied in this work the change of physical and chemical properties of Fe203-pillared clay. The pillared clay has been synthesized by intercalating polyoxycation of the iron into the interlayer of the montmorillortite clay. The intercalated compound then was calcinated at various temperature. They were 100°C, 150°C, 200°C, 250°C, and 300°C to obtain Fe203-pillared clay. The observed properties were basal spacing door, specific surface area, pore-size distribution, total pore volume, adsorption isotherm and surface acidity. The basal spacing door was determined by X-ray diffraction method, specific surface area, average pore radius, total pore volume and adsorption isotherm were analyzed by Gas Sorption Method Analysis, and surface acidity measured by gravimetric and FTIR Spectroscopic methods. The result of characterization showed that the basal spacing clan increament of Na-montmorillonite, Fe-PILCioo, Fe-PILC150, FePILC2oo, Fe-PILC23o, and Fe-PILC3oo were 6.05A, 7.99A, 22.97 A, 6.51A, and 10.18A, respectively. The specific surface area of Namontmorillonite, Fe-PILCtoo, Fe-PILCiso, Fe-PILC200, Fe-PILC2so, and Fe-PILC300 were 90.0587 m2/ g, 155.0751m2/g, 164.0924m2/g, 170.5416m2/g, 161.1349m2/g and 144.3453m2/g, respectively.The pore-size distribution is bimodal. The total pore volume of Namont and Fe-PILC were 0.06092 cc/ g and 0.12626 cc/ g to 0.15450 cc/ g. The N2 adsorption isotherm on Fe203 (Fe-PILC) are of type IV in the BDDT classification indicating that these pillared clay have both micropore and mesopore. The surface acidity of Namontmorillonite and Fe203 pillared clay were 0.5096 mmol/ g and 2.8498 mmol/ g to 7.0515 mmol/ g, respectively. Determination of Fe content showed that the average content of Fe203-Pillared Clay was 23,46 % w/w. Keyword : montmorillonite clay, calcinated,Fe203-Pillared Clay [Yogyakarta] : Universitas Gadjah Mada 2004 Article NonPeerReviewed Perpustakaan UGM, i-lib (2004) Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties. Jurnal i-lib UGM. http://i-lib.ugm.ac.id/jurnal/download.php?dataId=402
institution Universitas Gadjah Mada
building UGM Library
country Indonesia
collection Repository Civitas UGM
topic Jurnal i-lib UGM
spellingShingle Jurnal i-lib UGM
Perpustakaan UGM, i-lib
Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties
description It has been studied in this work the change of physical and chemical properties of Fe203-pillared clay. The pillared clay has been synthesized by intercalating polyoxycation of the iron into the interlayer of the montmorillortite clay. The intercalated compound then was calcinated at various temperature. They were 100°C, 150°C, 200°C, 250°C, and 300°C to obtain Fe203-pillared clay. The observed properties were basal spacing door, specific surface area, pore-size distribution, total pore volume, adsorption isotherm and surface acidity. The basal spacing door was determined by X-ray diffraction method, specific surface area, average pore radius, total pore volume and adsorption isotherm were analyzed by Gas Sorption Method Analysis, and surface acidity measured by gravimetric and FTIR Spectroscopic methods. The result of characterization showed that the basal spacing clan increament of Na-montmorillonite, Fe-PILCioo, Fe-PILC150, FePILC2oo, Fe-PILC23o, and Fe-PILC3oo were 6.05A, 7.99A, 22.97 A, 6.51A, and 10.18A, respectively. The specific surface area of Namontmorillonite, Fe-PILCtoo, Fe-PILCiso, Fe-PILC200, Fe-PILC2so, and Fe-PILC300 were 90.0587 m2/ g, 155.0751m2/g, 164.0924m2/g, 170.5416m2/g, 161.1349m2/g and 144.3453m2/g, respectively.The pore-size distribution is bimodal. The total pore volume of Namont and Fe-PILC were 0.06092 cc/ g and 0.12626 cc/ g to 0.15450 cc/ g. The N2 adsorption isotherm on Fe203 (Fe-PILC) are of type IV in the BDDT classification indicating that these pillared clay have both micropore and mesopore. The surface acidity of Namontmorillonite and Fe203 pillared clay were 0.5096 mmol/ g and 2.8498 mmol/ g to 7.0515 mmol/ g, respectively. Determination of Fe content showed that the average content of Fe203-Pillared Clay was 23,46 % w/w. Keyword : montmorillonite clay, calcinated,Fe203-Pillared Clay
format Article
NonPeerReviewed
author Perpustakaan UGM, i-lib
author_facet Perpustakaan UGM, i-lib
author_sort Perpustakaan UGM, i-lib
title Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties
title_short Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties
title_full Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties
title_fullStr Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties
title_full_unstemmed Sintesis lempung montmorillonit terpilar Fe2O3 dan kajian sifat-sfat kimia fisiknya=Synthesis of Fe2O3 pillared montmorillonite clay and study of its physico-chemical properties
title_sort sintesis lempung montmorillonit terpilar fe2o3 dan kajian sifat-sfat kimia fisiknya=synthesis of fe2o3 pillared montmorillonite clay and study of its physico-chemical properties
publisher [Yogyakarta] : Universitas Gadjah Mada
publishDate 2004
url https://repository.ugm.ac.id/17641/
http://i-lib.ugm.ac.id/jurnal/download.php?dataId=402
_version_ 1681217118700306432