Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure

Objectives: To evaluate the effect of simulated pulpal pressure (PP) on initial bond strength of one-stsep self-etch adhesives with different smear layer preparation. Methods: Flat coronal dentin surfaces were obtained from extracted molar teeth .Smear layers were created by grinding with either #18...

Full description

Saved in:
Bibliographic Details
Main Authors: Mahdan, Mohd. Haidil Akmal, Masatoshi, Nakajima, Junji, Tagami
Format: Conference or Workshop Item
Language:English
English
Published: 2012
Subjects:
Online Access:http://irep.iium.edu.my/44213/6/aadr2012.pdf
http://irep.iium.edu.my/44213/11/2012-aadrlist.pdf
http://irep.iium.edu.my/44213/
https://iadr.confex.com/iadr/2012tampa/webprogram/Paper156443.html
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universiti Islam Antarabangsa Malaysia
Language: English
English
id my.iium.irep.44213
record_format dspace
spelling my.iium.irep.442132015-11-30T07:14:50Z http://irep.iium.edu.my/44213/ Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure Mahdan, Mohd. Haidil Akmal Masatoshi, Nakajima Junji, Tagami RK Dentistry Objectives: To evaluate the effect of simulated pulpal pressure (PP) on initial bond strength of one-stsep self-etch adhesives with different smear layer preparation. Methods: Flat coronal dentin surfaces were obtained from extracted molar teeth .Smear layers were created by grinding with either #180 or #600 grit paper. A HEMA-free one-step self-etch adhesive, Xeno V (XV; Denstply,Germany) and a HEMA-containing adhesive, Tokuyama Bond Force (TBF;Tokuyama Corporation,Japan) were applied to the dentin surfaces according to the manufacturer's instructions under a hydrostatic pressure of 0 or 15 cmH2O. Specimens bonded under 0 cmH20 pressure was served as a control group. After coronal build up with composite resin (CLEARFIL AP-X), the specimens were stored in water at 370C for 24 hour. Bond strength to dentin were determined using microtensile bond (TBS) testing and all data were statistically analyzed using one-way ANOVA (materials and experimental conditions) and additional t-test. Results: The bond strength values (TBS) results table are as follows. Bond Strength of HEMA-free And HEMA-containing Adhesives Under Pulpal Pressure. Available from: http://www.researchgate.net/publication/266777476_Bond_Strength_of_HEMA-free_And_HEMA-containing_Adhesives_Under_Pulpal_Pressure [accessed Dec 1, 2015]. 2012 Conference or Workshop Item REM application/pdf en http://irep.iium.edu.my/44213/6/aadr2012.pdf application/pdf en http://irep.iium.edu.my/44213/11/2012-aadrlist.pdf Mahdan, Mohd. Haidil Akmal and Masatoshi, Nakajima and Junji, Tagami (2012) Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure. In: American Asoociation of Dental Research 2012 (AADR Annual Meeting), 21-24 March 2012, Tampa,USA. (Unpublished) https://iadr.confex.com/iadr/2012tampa/webprogram/Paper156443.html
institution Universiti Islam Antarabangsa Malaysia
building IIUM Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider International Islamic University Malaysia
content_source IIUM Repository (IREP)
url_provider http://irep.iium.edu.my/
language English
English
topic RK Dentistry
spellingShingle RK Dentistry
Mahdan, Mohd. Haidil Akmal
Masatoshi, Nakajima
Junji, Tagami
Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
description Objectives: To evaluate the effect of simulated pulpal pressure (PP) on initial bond strength of one-stsep self-etch adhesives with different smear layer preparation. Methods: Flat coronal dentin surfaces were obtained from extracted molar teeth .Smear layers were created by grinding with either #180 or #600 grit paper. A HEMA-free one-step self-etch adhesive, Xeno V (XV; Denstply,Germany) and a HEMA-containing adhesive, Tokuyama Bond Force (TBF;Tokuyama Corporation,Japan) were applied to the dentin surfaces according to the manufacturer's instructions under a hydrostatic pressure of 0 or 15 cmH2O. Specimens bonded under 0 cmH20 pressure was served as a control group. After coronal build up with composite resin (CLEARFIL AP-X), the specimens were stored in water at 370C for 24 hour. Bond strength to dentin were determined using microtensile bond (TBS) testing and all data were statistically analyzed using one-way ANOVA (materials and experimental conditions) and additional t-test. Results: The bond strength values (TBS) results table are as follows. Bond Strength of HEMA-free And HEMA-containing Adhesives Under Pulpal Pressure. Available from: http://www.researchgate.net/publication/266777476_Bond_Strength_of_HEMA-free_And_HEMA-containing_Adhesives_Under_Pulpal_Pressure [accessed Dec 1, 2015].
format Conference or Workshop Item
author Mahdan, Mohd. Haidil Akmal
Masatoshi, Nakajima
Junji, Tagami
author_facet Mahdan, Mohd. Haidil Akmal
Masatoshi, Nakajima
Junji, Tagami
author_sort Mahdan, Mohd. Haidil Akmal
title Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
title_short Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
title_full Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
title_fullStr Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
title_full_unstemmed Bond strength of HEMA-free and HEMA-containing adhesives under pulpal pressure
title_sort bond strength of hema-free and hema-containing adhesives under pulpal pressure
publishDate 2012
url http://irep.iium.edu.my/44213/6/aadr2012.pdf
http://irep.iium.edu.my/44213/11/2012-aadrlist.pdf
http://irep.iium.edu.my/44213/
https://iadr.confex.com/iadr/2012tampa/webprogram/Paper156443.html
_version_ 1643612533178761216