Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc

Surface alloying with ceramic powder uses a high energy input to create composite coating that provides protection against wear and corrosion. In this work TiC incorporated composite coating was created by melting single tracks in 1.0 mg/mm2 TiC powder preplaced on alloy steel surfaces using a conve...

Full description

Saved in:
Bibliographic Details
Main Authors: Mridha, Shahjahan, Md. Idriss, A. N., Maleque, Md. Abdul, -, Suryanto, Mohamad, Souad A.
Format: Conference or Workshop Item
Language:English
Published: 2011
Subjects:
Online Access:http://irep.iium.edu.my/7341/1/RTC074.pdf
http://irep.iium.edu.my/7341/
http://www.mytribos.org/rtc2011
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universiti Islam Antarabangsa Malaysia
Language: English
id my.iium.irep.7341
record_format dspace
spelling my.iium.irep.73412011-12-02T07:07:38Z http://irep.iium.edu.my/7341/ Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc Mridha, Shahjahan Md. Idriss, A. N. Maleque, Md. Abdul -, Suryanto Mohamad, Souad A. TN Mining engineering. Metallurgy TS Manufactures Surface alloying with ceramic powder uses a high energy input to create composite coating that provides protection against wear and corrosion. In this work TiC incorporated composite coating was created by melting single tracks in 1.0 mg/mm2 TiC powder preplaced on alloy steel surfaces using a conventional TIG welding torch produced at 80 ampere current with a voltage between 30 to 55V and a constant traversing speed of 1.0 mm/s. The effect of voltage, used to generate TIG torch for melting, was investigated in terms of geometry, microstructure and hardness of the processed track. The TIG torch produced with different voltages created melt pool of hemispherical shape with varying track dimensions. The melt dimensions increased with increasing voltage. Glazing with 30 V created a melt pool of 3.10mm wide and 0.80 mm deep; the maximum width of 3.96mm and depth of 0.97 mm was produced at 55 V and 45 V, respectively. Tracks produced under different conditions were free from cracks but pores were seen in places. The melt microstructures consisted of partially dissolved and unmelted TiC particulates along with dendrites of a variety of TiC precipitates. Agglomeration of TiC was apparent at the edges. The population of TiC precipitates and partially dissolved TiC particulates increased when glazed at high voltage torch. Hardness development was lowest when glazed at 30 V and it increased by glazing at 35 and 45 V. The population of TiC particulates and their sizes were seen to influence the hardness and this phenomenon is also similar for the precipitated particlesHardness development was lowest when glazed at 30 V and it increased by glazing at 35 and 45 V. The population of TiC particulates and their sizes were seen to influence the hardness and this phenomenon is also similar for the precipitated particles. 2011-11 Conference or Workshop Item REM application/pdf en http://irep.iium.edu.my/7341/1/RTC074.pdf Mridha, Shahjahan and Md. Idriss, A. N. and Maleque, Md. Abdul and -, Suryanto and Mohamad, Souad A. (2011) Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc. In: Regional Tribology Conference 2011, 22-24 November 2011, Langkawi, Malaysia. http://www.mytribos.org/rtc2011
institution Universiti Islam Antarabangsa Malaysia
building IIUM Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider International Islamic University Malaysia
content_source IIUM Repository (IREP)
url_provider http://irep.iium.edu.my/
language English
topic TN Mining engineering. Metallurgy
TS Manufactures
spellingShingle TN Mining engineering. Metallurgy
TS Manufactures
Mridha, Shahjahan
Md. Idriss, A. N.
Maleque, Md. Abdul
-, Suryanto
Mohamad, Souad A.
Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc
description Surface alloying with ceramic powder uses a high energy input to create composite coating that provides protection against wear and corrosion. In this work TiC incorporated composite coating was created by melting single tracks in 1.0 mg/mm2 TiC powder preplaced on alloy steel surfaces using a conventional TIG welding torch produced at 80 ampere current with a voltage between 30 to 55V and a constant traversing speed of 1.0 mm/s. The effect of voltage, used to generate TIG torch for melting, was investigated in terms of geometry, microstructure and hardness of the processed track. The TIG torch produced with different voltages created melt pool of hemispherical shape with varying track dimensions. The melt dimensions increased with increasing voltage. Glazing with 30 V created a melt pool of 3.10mm wide and 0.80 mm deep; the maximum width of 3.96mm and depth of 0.97 mm was produced at 55 V and 45 V, respectively. Tracks produced under different conditions were free from cracks but pores were seen in places. The melt microstructures consisted of partially dissolved and unmelted TiC particulates along with dendrites of a variety of TiC precipitates. Agglomeration of TiC was apparent at the edges. The population of TiC precipitates and partially dissolved TiC particulates increased when glazed at high voltage torch. Hardness development was lowest when glazed at 30 V and it increased by glazing at 35 and 45 V. The population of TiC particulates and their sizes were seen to influence the hardness and this phenomenon is also similar for the precipitated particlesHardness development was lowest when glazed at 30 V and it increased by glazing at 35 and 45 V. The population of TiC particulates and their sizes were seen to influence the hardness and this phenomenon is also similar for the precipitated particles.
format Conference or Workshop Item
author Mridha, Shahjahan
Md. Idriss, A. N.
Maleque, Md. Abdul
-, Suryanto
Mohamad, Souad A.
author_facet Mridha, Shahjahan
Md. Idriss, A. N.
Maleque, Md. Abdul
-, Suryanto
Mohamad, Souad A.
author_sort Mridha, Shahjahan
title Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc
title_short Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc
title_full Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc
title_fullStr Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc
title_full_unstemmed Effect of voltage on the consolidation of tic particulates on steel substrate fused by TIG welding arc
title_sort effect of voltage on the consolidation of tic particulates on steel substrate fused by tig welding arc
publishDate 2011
url http://irep.iium.edu.my/7341/1/RTC074.pdf
http://irep.iium.edu.my/7341/
http://www.mytribos.org/rtc2011
_version_ 1643605920357285888