Sintered strength of ti-6Al-4V by metal injection molding (MIM) using palm stearin binder / N. H. Mohamad Nor...[et al.]
Metal injection molding (MIM) is a metal working process used to compact Titanium, Ti-6Al-4V and the binder through injection moulding process. In this work, Titanium Ti-6Al-4V was mixed with palm stearin (PS) and polyethylene (PE) which act as a binder. Palm stearin (PS) is a potential binder syste...