Optimization of sintering temperature for the enhancement of pyroelectric properties of lead-free 0.88(Na 0.5 Bi 0.5 )TiO 3 –0.084(K 0.5 Bi 0.5 )TiO 3 –0.036BaTiO 3 piezoelectric ceramics
Lead-free 0.88(Na0.5Bi0.5)TiO3–0.084(K0.5Bi0.5)TiO3–0.036BaTiO3 (BNT–BKT–BT) piezoelectric ceramics were prepared using the conventional mixed-oxide method with a sintering temperature range of 1120–1200 °C. The effect of the sintering temperature on the crystal structure, microstructure, and densif...