Development of hot stamping tool by using indirect hot stamping for basic bending part (u-shape)
In hot stamping process, (UHSS) blank was cut into the rough shape. The blank is then heated to the temperature (900 - 950 °C) for 5 to 10 minutes inside the furnace. Then, the blank must be transferred quickly to the press to avoid the part is cooled before forming. After that, the blank is formed...