Permanent Deformation of Hot Mix Asphalt (HMA) using Dynamic Modulus Simple Performance Test
Premature pavement breakdown can be caused by permanent deformation that can contribute to lower riding comfort for road users and an increase in maintenance costs. Dynamic modulus Simple Performance Test (SPT) test are considered to be significant in describing the permanent deformation of hot mix...