Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding

The present study focuses on the effects of material position and tool rotational speed on the tensile strength of dissimilar AA7071 and AA6061 welded aluminum alloys with a thickness of 2.0 mm in using a conventional milling machine. Ten joints were produced by varying tool rotational speeds and by...

Full description

Saved in:
Bibliographic Details
Main Authors: N. A. A., Sathari, A. R., Razali, M., Ishak, L. H., Shah
Format: Article
Language:English
Published: Universiti Malaysia Pahang 2015
Subjects:
Online Access:http://umpir.ump.edu.my/id/eprint/9873/1/Mechanical%20Strength%20Of%20Dissimilar%20AA7075%20and%20AA6061%20Aluminum%20Alloys%20Using%20Friction%20Stir%20Welding.pdf
http://umpir.ump.edu.my/id/eprint/9873/
http://ijame.ump.edu.my/images/Volume_11%20June%202015/47_Sathari%20et%20al.pdf
http://dx.doi.org/10.15282/ijame.11.2015.47.022
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universiti Malaysia Pahang
Language: English
id my.ump.umpir.9873
record_format eprints
spelling my.ump.umpir.98732018-01-10T03:16:20Z http://umpir.ump.edu.my/id/eprint/9873/ Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding N. A. A., Sathari A. R., Razali M., Ishak L. H., Shah TJ Mechanical engineering and machinery The present study focuses on the effects of material position and tool rotational speed on the tensile strength of dissimilar AA7071 and AA6061 welded aluminum alloys with a thickness of 2.0 mm in using a conventional milling machine. Ten joints were produced by varying tool rotational speeds and by changing the fixed position of the material on the advancing and retreating sides. The results show that the maximum tensile strength of 207 MPa was achieved for Sample E when AA6061 aluminum alloys were placed on the advancing side at a rotational speed of 1000 rpm with seamless surface appearance and no inner defect across the weld area, while the lowest tensile strength of 160 MPa was obtained for Sample F when AA6061 was placed on the retreating side with severe tunnel defects across the weld area contributing to crack propagation. Thus, in dissimilar welding, weaker materials should be placed on the advancing side to trigger heat from the tool rotation and smooth the material flow formation in the stirred zone. Universiti Malaysia Pahang 2015 Article PeerReviewed application/pdf en cc_by http://umpir.ump.edu.my/id/eprint/9873/1/Mechanical%20Strength%20Of%20Dissimilar%20AA7075%20and%20AA6061%20Aluminum%20Alloys%20Using%20Friction%20Stir%20Welding.pdf N. A. A., Sathari and A. R., Razali and M., Ishak and L. H., Shah (2015) Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding. International Journal of Automotive and Mechanical Engineering (IJAME), 11. pp. 2713-2721. ISSN 1985-9325(Print); 2180-1606 (Online) http://ijame.ump.edu.my/images/Volume_11%20June%202015/47_Sathari%20et%20al.pdf http://dx.doi.org/10.15282/ijame.11.2015.47.022
institution Universiti Malaysia Pahang
building UMP Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Malaysia Pahang
content_source UMP Institutional Repository
url_provider http://umpir.ump.edu.my/
language English
topic TJ Mechanical engineering and machinery
spellingShingle TJ Mechanical engineering and machinery
N. A. A., Sathari
A. R., Razali
M., Ishak
L. H., Shah
Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding
description The present study focuses on the effects of material position and tool rotational speed on the tensile strength of dissimilar AA7071 and AA6061 welded aluminum alloys with a thickness of 2.0 mm in using a conventional milling machine. Ten joints were produced by varying tool rotational speeds and by changing the fixed position of the material on the advancing and retreating sides. The results show that the maximum tensile strength of 207 MPa was achieved for Sample E when AA6061 aluminum alloys were placed on the advancing side at a rotational speed of 1000 rpm with seamless surface appearance and no inner defect across the weld area, while the lowest tensile strength of 160 MPa was obtained for Sample F when AA6061 was placed on the retreating side with severe tunnel defects across the weld area contributing to crack propagation. Thus, in dissimilar welding, weaker materials should be placed on the advancing side to trigger heat from the tool rotation and smooth the material flow formation in the stirred zone.
format Article
author N. A. A., Sathari
A. R., Razali
M., Ishak
L. H., Shah
author_facet N. A. A., Sathari
A. R., Razali
M., Ishak
L. H., Shah
author_sort N. A. A., Sathari
title Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding
title_short Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding
title_full Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding
title_fullStr Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding
title_full_unstemmed Mechanical Strength Of Dissimilar AA7075 and AA6061 Aluminum Alloys Using Friction Stir Welding
title_sort mechanical strength of dissimilar aa7075 and aa6061 aluminum alloys using friction stir welding
publisher Universiti Malaysia Pahang
publishDate 2015
url http://umpir.ump.edu.my/id/eprint/9873/1/Mechanical%20Strength%20Of%20Dissimilar%20AA7075%20and%20AA6061%20Aluminum%20Alloys%20Using%20Friction%20Stir%20Welding.pdf
http://umpir.ump.edu.my/id/eprint/9873/
http://ijame.ump.edu.my/images/Volume_11%20June%202015/47_Sathari%20et%20al.pdf
http://dx.doi.org/10.15282/ijame.11.2015.47.022
_version_ 1643666242985263104