Effect of nanofillers in jute/carbon hybrid reinforced polylactic acid composite
The presence of fibres and fillers in a composite can be efficiently arrest crack either at the macro or micro levels. In this work, woven jute and carbon fibres were arranged alternately in polylactic acid (PLA) composite. Graphene or nanoclay was embedded into the PLA matrix to make a polymer n...
Saved in:
Main Author: | |
---|---|
Format: | Thesis |
Language: | English |
Published: |
2021
|
Subjects: | |
Online Access: | http://psasir.upm.edu.my/id/eprint/104120/1/NUR%20AQILAH%20BINTI%20SAIRY%20-%20IR.pdf http://psasir.upm.edu.my/id/eprint/104120/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Putra Malaysia |
Language: | English |
Summary: | The presence of fibres and fillers in a composite can be efficiently arrest crack
either at the macro or micro levels. In this work, woven jute and carbon fibres
were arranged alternately in polylactic acid (PLA) composite. Graphene or
nanoclay was embedded into the PLA matrix to make a polymer nanocomposite.
Fibre-reinforced polymer composites were prepared by varying the
concentration (1, 3, 5wt%) of graphene or nanoclay in the PLA matrix. The
alternate woven jute and carbon fibres aere then bound with the PLA
nanocomposite. The influence of graphene or nanoclay concentration and the
presence of woven fibres in the composite were quantified by flexural analysis.
Flexural strength and flexural modulus were found to increase at 3wt% of
nanofiller concentration for graphene/jute/PLA and nanoclay/jute/PLA
nanocomposites with the increments up to 37% and 31%, respectively. Lowvelocity
impact revealed that PLA/TJ/C/G1, PLA/TJ/C/G3, and PLA/TJ/C/G1
have the highest force value for 7J, 10J, and 13J, respectively. These three
optimum values for each energy indicate that the closed curve results from the
striker’s inability to penetrate the specimen. Thus, it was assumed that the lower
loading of graphene could withstand the impact energy of 7J, 10J, and 13J. FTIR
was used to determine the interaction between PLA and nanofillers. Morphology
observation by Scanning Electron Microscopy (SEM) was done to investigate the
fractured surface of the hybrid jute/carbon fibres reinforced PLA nanocomposite. |
---|