Sifat transmisi, pekali pupusan dan keterpantulan optik kepingan poli(metil metakrilat) (PMMA) didop dengan metil merah dan ferum (III) asetilasetonat
The optical transmission, reflection and extinction coefficient of a PMMA doped with methylene-red (PMMA-MM) and ferum (III) acetylacetonate (PMMA-FM) are presented. A rapid change of the optical transmission was observed in the range of wavelength (420-650 nm) and (500 - 600nm) for PMMA-FM and PMMA...
Saved in:
Main Authors: | , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Universiti Putra Malaysia Press
1999
|
Online Access: | http://psasir.upm.edu.my/id/eprint/3493/1/Sifat_Transmisi%2C_Pekali_Pupusan_dan_Keterpantulan_Optik.pdf http://psasir.upm.edu.my/id/eprint/3493/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Putra Malaysia |
Language: | English |
Summary: | The optical transmission, reflection and extinction coefficient of a PMMA doped with methylene-red (PMMA-MM) and ferum (III) acetylacetonate (PMMA-FM) are presented. A rapid change of the optical transmission was observed in the range of wavelength (420-650 nm) and (500 - 600nm) for PMMA-FM and PMMAMM respectively. Eventhough the decrease of the optical transmission and the increase of the extinction coefficient do not linearly relate with increasing
concentration of methylene-red and ferum (III) asetilasetonate, the transmission curve and the cut off transmission are still affected by doping concentration. It
was found that the cut off value for PMMA-MM shifted from 200nm (for pure PMMA) to 550 nm when the concentration was increased to 6.3 31O-3mmol/g. A similar shift (200nm to 500nm) was also observed for PMMA-FM but with a higher doping concentration (i.e 30.7310-3 mmol/g). |
---|