Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process

The recovery of gold from gold-copper and gold-cobalt cyanide based electroplating solutions using an electrogenerative process was carried out with a batch cell. The cathodes that had been used for this studied were porous graphite and reticulated vitreous carbon (RVC) while for anode was zinc foil...

Full description

Saved in:
Bibliographic Details
Main Author: Aminuddin, Norazlina
Format: Thesis
Language:English
Published: 2011
Subjects:
Online Access:http://eprints.usm.my/40907/1/Norazlina_Bt_Aminuddin_24MS_HJ.pdf
http://eprints.usm.my/40907/
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universiti Sains Malaysia
Language: English
id my.usm.eprints.40907
record_format eprints
spelling my.usm.eprints.40907 http://eprints.usm.my/40907/ Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process Aminuddin, Norazlina QD1-999 Chemistry The recovery of gold from gold-copper and gold-cobalt cyanide based electroplating solutions using an electrogenerative process was carried out with a batch cell. The cathodes that had been used for this studied were porous graphite and reticulated vitreous carbon (RVC) while for anode was zinc foil. The influence of the presence of copper and cobalt metal ions toward gold deposition was studied by cyclic voltammetry. The recovery studies were carried out for 6 hours during which the gold in the bath solutions was determined by atomic absorption spectroscopy at regular intervals. The surface morphology and purity of the deposited gold were determined using scanning electron microscopy – energy dispersive X-ray spectrometry (SEM-EDX). More than 99% of gold was recovered after 6 h of operation using non-activated cathodes. It takes 3 h to recover more than 99 % of gold using activated cathodes. Activated RVC is a superior cathode material having the highest recovery rate compared to activated porous graphite, stainless steel and copper sheet. More gold is recovered when using a greater electrode surface area that is exposed to the catholyte solution. The results also show that at pH greater than 10 and with higher free cyanide concentration, copper will not be co-deposited with the gold. 2011-03 Thesis NonPeerReviewed application/pdf en http://eprints.usm.my/40907/1/Norazlina_Bt_Aminuddin_24MS_HJ.pdf Aminuddin, Norazlina (2011) Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process. Masters thesis, Universiti Sains Malaysia.
institution Universiti Sains Malaysia
building Hamzah Sendut Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Sains Malaysia
content_source USM Institutional Repository
url_provider http://eprints.usm.my/
language English
topic QD1-999 Chemistry
spellingShingle QD1-999 Chemistry
Aminuddin, Norazlina
Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process
description The recovery of gold from gold-copper and gold-cobalt cyanide based electroplating solutions using an electrogenerative process was carried out with a batch cell. The cathodes that had been used for this studied were porous graphite and reticulated vitreous carbon (RVC) while for anode was zinc foil. The influence of the presence of copper and cobalt metal ions toward gold deposition was studied by cyclic voltammetry. The recovery studies were carried out for 6 hours during which the gold in the bath solutions was determined by atomic absorption spectroscopy at regular intervals. The surface morphology and purity of the deposited gold were determined using scanning electron microscopy – energy dispersive X-ray spectrometry (SEM-EDX). More than 99% of gold was recovered after 6 h of operation using non-activated cathodes. It takes 3 h to recover more than 99 % of gold using activated cathodes. Activated RVC is a superior cathode material having the highest recovery rate compared to activated porous graphite, stainless steel and copper sheet. More gold is recovered when using a greater electrode surface area that is exposed to the catholyte solution. The results also show that at pH greater than 10 and with higher free cyanide concentration, copper will not be co-deposited with the gold.
format Thesis
author Aminuddin, Norazlina
author_facet Aminuddin, Norazlina
author_sort Aminuddin, Norazlina
title Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process
title_short Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process
title_full Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process
title_fullStr Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process
title_full_unstemmed Recovery Of Gold From Gold-Copper And Gold-Cobalt Cyanide Based Electroplating Solutions By Using An Electrogenerative Process
title_sort recovery of gold from gold-copper and gold-cobalt cyanide based electroplating solutions by using an electrogenerative process
publishDate 2011
url http://eprints.usm.my/40907/1/Norazlina_Bt_Aminuddin_24MS_HJ.pdf
http://eprints.usm.my/40907/
_version_ 1643710072255152128