Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials
A serious need for a robust, low-cost and eco-friendly method to treat dye pollutants released by textile industries motivated this research. The dye adsorption effect of biodegradable poly-3-hydroxybutyrate [P(3HB)] and the photocatalytic degradation ability of inert titanium dioxide (TiO2) was exp...
Saved in:
Main Author: | |
---|---|
Format: | Thesis |
Language: | English |
Published: |
2012
|
Subjects: | |
Online Access: | http://eprints.usm.my/45871/1/NANTHINI%20SRIDEWI%20%20APPAN_HJ.pdf http://eprints.usm.my/45871/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Sains Malaysia |
Language: | English |
id |
my.usm.eprints.45871 |
---|---|
record_format |
eprints |
spelling |
my.usm.eprints.45871 http://eprints.usm.my/45871/ Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials Appan, Nanthini Sridewi QH1 Natural history (General - Including nature conservation, geographical distribution) A serious need for a robust, low-cost and eco-friendly method to treat dye pollutants released by textile industries motivated this research. The dye adsorption effect of biodegradable poly-3-hydroxybutyrate [P(3HB)] and the photocatalytic degradation ability of inert titanium dioxide (TiO2) was exploited to fabricate a multifunctional nanocomposite film via solvent casting and electrospinning. The environmental degradation of the choice material, cast P(3HB) was first tested and confirmed to be comparable to its co-polymers; poly(3-hydroxybutyrate-co-5 mol% 3-hydroxyvalerate) [P(3HB-co-5 mol% 3HV)] and poly(3-hydroxybutyrate-co-5 mol% 3-hydroxyhexanoate) [P(3HB-co-5 mol% 3HHx)]. The weight loss was almost complete by 8 weeks in tropical mangrove sediment. The nanocomposite film was also degradable although to a lesser extent despite the microbial inactivation effect of TiO2. The optimum amount of P(3HB) and TiO2 loading in cast film was found to be 0.4 g and 40 wt% respectively. This film had an even distribution of TiO2 when mixed concurrently in chloroform followed by stirring for 24 h. It completely decolorized and detoxified real industrial Batik dye wastewater in 3 h and induced a chemical oxygen demand (COD) reduction of 80%. The 0.4 g P(3HB)-40 wt% TiO2 film exhibited good stability with decolorization percentage of ≥80% even after the sixth repeated usage. 2012-02 Thesis NonPeerReviewed application/pdf en http://eprints.usm.my/45871/1/NANTHINI%20SRIDEWI%20%20APPAN_HJ.pdf Appan, Nanthini Sridewi (2012) Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials. PhD thesis, Universiti Sains Malaysia. |
institution |
Universiti Sains Malaysia |
building |
Hamzah Sendut Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Sains Malaysia |
content_source |
USM Institutional Repository |
url_provider |
http://eprints.usm.my/ |
language |
English |
topic |
QH1 Natural history (General - Including nature conservation, geographical distribution) |
spellingShingle |
QH1 Natural history (General - Including nature conservation, geographical distribution) Appan, Nanthini Sridewi Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials |
description |
A serious need for a robust, low-cost and eco-friendly method to treat dye pollutants released by textile industries motivated this research. The dye adsorption effect of biodegradable poly-3-hydroxybutyrate [P(3HB)] and the photocatalytic degradation ability of inert titanium dioxide (TiO2) was exploited to fabricate a multifunctional nanocomposite film via solvent casting and electrospinning. The environmental degradation of the choice material, cast P(3HB) was first tested and confirmed to be comparable to its co-polymers; poly(3-hydroxybutyrate-co-5 mol% 3-hydroxyvalerate) [P(3HB-co-5 mol% 3HV)] and poly(3-hydroxybutyrate-co-5 mol% 3-hydroxyhexanoate) [P(3HB-co-5 mol% 3HHx)]. The weight loss was almost complete by 8 weeks in tropical mangrove sediment. The nanocomposite film was also degradable although to a lesser extent despite the microbial inactivation effect of TiO2. The optimum amount of P(3HB) and TiO2 loading in cast film was found to be 0.4 g and 40 wt% respectively. This film had an even distribution of TiO2 when mixed concurrently in chloroform followed by stirring for 24 h. It completely decolorized and detoxified real industrial Batik dye wastewater in 3 h and induced a chemical oxygen demand (COD) reduction of 80%. The 0.4 g P(3HB)-40 wt% TiO2 film exhibited good stability with decolorization percentage of ≥80% even after the sixth repeated usage. |
format |
Thesis |
author |
Appan, Nanthini Sridewi |
author_facet |
Appan, Nanthini Sridewi |
author_sort |
Appan, Nanthini Sridewi |
title |
Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials |
title_short |
Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials |
title_full |
Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials |
title_fullStr |
Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials |
title_full_unstemmed |
Fabrication, Characterization And Application Of Polyhydroxybutyrate-Titanium Dioxide Nanocomposite Materials |
title_sort |
fabrication, characterization and application of polyhydroxybutyrate-titanium dioxide nanocomposite materials |
publishDate |
2012 |
url |
http://eprints.usm.my/45871/1/NANTHINI%20SRIDEWI%20%20APPAN_HJ.pdf http://eprints.usm.my/45871/ |
_version_ |
1657488779997347840 |