Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation
Silver sulfate (Ag2S04) was successfully deposited on ZnO via a simple impregnation method. The as-synthesized sample was characterized by XRD, SEM, TEM, EDX, FTIR, UV-vis DRS and BET surface characteristic. Then, the photocatalytic activities of pure ZnO and three Ag2S04-deposited ZnO with diffe...
Saved in:
Main Author: | |
---|---|
Format: | Thesis |
Language: | English |
Published: |
2014
|
Subjects: | |
Online Access: | http://eprints.usm.my/61136/1/24%20Pages%20from%2000001785143.pdf http://eprints.usm.my/61136/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Sains Malaysia |
Language: | English |
id |
my.usm.eprints.61136 |
---|---|
record_format |
eprints |
spelling |
my.usm.eprints.61136 http://eprints.usm.my/61136/ Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation Choo, Hui Sun TP1-1185 Chemical technology Silver sulfate (Ag2S04) was successfully deposited on ZnO via a simple impregnation method. The as-synthesized sample was characterized by XRD, SEM, TEM, EDX, FTIR, UV-vis DRS and BET surface characteristic. Then, the photocatalytic activities of pure ZnO and three Ag2S04-deposited ZnO with different Ag2S04 loading were being evaluated for the degradation of indigo carmine and phenol under outdoor light irradiation. Results showed that the photocatalytic activities of all theer Ag2S04-deposited ZnO were higher than pure ZnO and commercial Ti02 for both pollutants degradation, especially 0.03 Ag2S04/ZnO which exhibited superior photocatalytic performance compare to others. After that, calcination temperature at 300 oe was found to be the most suitable condition for the preparation of 0.03 Ag2S0 2014-12 Thesis NonPeerReviewed application/pdf en http://eprints.usm.my/61136/1/24%20Pages%20from%2000001785143.pdf Choo, Hui Sun (2014) Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation. Masters thesis, Perpustakaan Hamzah Sendut. |
institution |
Universiti Sains Malaysia |
building |
Hamzah Sendut Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Sains Malaysia |
content_source |
USM Institutional Repository |
url_provider |
http://eprints.usm.my/ |
language |
English |
topic |
TP1-1185 Chemical technology |
spellingShingle |
TP1-1185 Chemical technology Choo, Hui Sun Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation |
description |
Silver sulfate (Ag2S04) was successfully deposited on ZnO via a simple
impregnation method. The as-synthesized sample was characterized by XRD, SEM,
TEM, EDX, FTIR, UV-vis DRS and BET surface characteristic. Then, the
photocatalytic activities of pure ZnO and three Ag2S04-deposited ZnO with different
Ag2S04 loading were being evaluated for the degradation of indigo carmine and
phenol under outdoor light irradiation. Results showed that the photocatalytic
activities of all theer Ag2S04-deposited ZnO were higher than pure ZnO and
commercial Ti02 for both pollutants degradation, especially 0.03 Ag2S04/ZnO which
exhibited superior photocatalytic performance compare to others. After that,
calcination temperature at 300 oe was found to be the most suitable condition for the
preparation of 0.03 Ag2S0 |
format |
Thesis |
author |
Choo, Hui Sun |
author_facet |
Choo, Hui Sun |
author_sort |
Choo, Hui Sun |
title |
Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation |
title_short |
Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation |
title_full |
Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation |
title_fullStr |
Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation |
title_full_unstemmed |
Photocatalytic Degradation Of Indigo Carmine And Phenol Using Agzs04-Deposited Zno Under Outdoor Light Irradiation |
title_sort |
photocatalytic degradation of indigo carmine and phenol using agzs04-deposited zno under outdoor light irradiation |
publishDate |
2014 |
url |
http://eprints.usm.my/61136/1/24%20Pages%20from%2000001785143.pdf http://eprints.usm.my/61136/ |
_version_ |
1811683105562427392 |