Evaluation of deep eutectic solvent as a new monomer for molecularly imprinted polymers for removal of bisphenol A
Deep eutectic solvent molecularly imprinted polymer (DES-MIP) was synthesized by bulk polymerization via free radical polymerization using bisphenol A (BPA) as a template, DES as a functional monomer, ethylene glycol dimethyl acrylate (EGDMA) as a crosslinker and benzoyl peroxide as initiator. DES...
Saved in:
Main Authors: | , |
---|---|
Format: | Article |
Language: | English |
Published: |
Springer
2023
|
Subjects: | |
Online Access: | http://eprints.uthm.edu.my/9959/1/J16059_93fd905aa81199ba88793e2a5b874707.pdf http://eprints.uthm.edu.my/9959/ https://doi.org/10.1007/s10965-023-03581-1 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Tun Hussein Onn Malaysia |
Language: | English |
Summary: | Deep eutectic solvent molecularly imprinted polymer (DES-MIP) was synthesized by bulk polymerization via free radical
polymerization using bisphenol A (BPA) as a template, DES as a functional monomer, ethylene glycol dimethyl acrylate
(EGDMA) as a crosslinker and benzoyl peroxide as initiator. DES functional monomer was prepared by the combination of choline chloride methacrylic acid (ChCl-MAA). The synthesized DES-MIP was then compared with conventional
molecularly imprinted polymer (MIP) synthesized using methacrylic acid (MAA) as a functional monomer. The DES-MIP has a higher selectivity for BPA (17.72 mg/g) than competing chemicals, including bisphenol AP (9.78 mg/g), 2-naphthol (8.25), and 4-tertiary butyl-phenol (6.98 mg/g). The optimization parameters include the effects of pH, adsorption kinetics, adsorption isotherm, and thermodynamic studies were investigated. DES-MIP showed the highest binding capacity at pH 7. The kinetic and isotherm studies demonstrated good agreement with a pseudo-second-order kinetic model and Langmuir isotherm models, respectively. The thermodynamic study proved that the adsorption of BPA on DES-MIP was exothermic and spontaneous with ΔH0
(-23.734×kJ/mol) and ΔG0 (-2.929 kJ/mol−). Reusability experiments show that the DES-MIP can be recycled five times without significantly diminishing its adsorption capacity. As a result, it proved that the contribution of DES as a functional monomer alternative in MIP synthesis considerably improved the recognition of BPA adsorption. |
---|