Effect of triple tempering temperature on microstructure, mechanical, and wear properties of K340 cold work tool steel.
The effect of triple tempering temperature (500-580 °C) on microstructure and properties of K340 steel, a new generation of the high Cr cold work tool steel, was investigated. Applied heat treatment consisted of preheating at 400, 600, and 800 °C for 20 min and consequently austenitizing at 1050 °C...