Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method

Sintering parameters of the SS316L water atomised injection moulded compact has been optimized for its best sintered density. The L9 (34) Taguchi orthogonal array is used in the experiment while sintering temperature, sintering time, heating rate and coofing rate was selected as factors that influen...

Full description

Saved in:
Bibliographic Details
Main Authors: Jamaludin, K. R., Muhamad, N., Ab. Rahman, M. N., M. Amin, S. Y., Ahmad, S., Ibrahim, M. H. I.
Format: Conference or Workshop Item
Language:English
Published: 2009
Subjects:
Online Access:http://eprints.utm.my/id/eprint/12620/1/KRJamaludin2008_SinteringParameterOptimisationoftheSS316LMetal.pdf
http://eprints.utm.my/id/eprint/12620/
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universiti Teknologi Malaysia
Language: English
id my.utm.12620
record_format eprints
spelling my.utm.126202011-06-14T07:42:22Z http://eprints.utm.my/id/eprint/12620/ Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method Jamaludin, K. R. Muhamad, N. Ab. Rahman, M. N. M. Amin, S. Y. Ahmad, S. Ibrahim, M. H. I. TJ Mechanical engineering and machinery TS Manufactures Sintering parameters of the SS316L water atomised injection moulded compact has been optimized for its best sintered density. The L9 (34) Taguchi orthogonal array is used in the experiment while sintering temperature, sintering time, heating rate and coofing rate was selected as factors that influenced the sintered density. The sintering environment was in the vacuum and four replications were done for each trial. The analysis of variance shows that the confident level for the experiment was 99.5 % (a = 0.005) and all factors are highly significant at a =0.005 to the sintered density. The study concluded that the heating rate has the highest influence to the sintered density (41.29 %) followed by sintering temperature (31.60 %) , sintering time (11.13 %) and cooling rate (11.10%). The optimum sintered density obtained is 98.48 % of the theoretical density and the optimum parameter has been verified that the sintered density obtained is in a range of confident interval. 2009-02 Conference or Workshop Item PeerReviewed application/pdf en http://eprints.utm.my/id/eprint/12620/1/KRJamaludin2008_SinteringParameterOptimisationoftheSS316LMetal.pdf Jamaludin, K. R. and Muhamad, N. and Ab. Rahman, M. N. and M. Amin, S. Y. and Ahmad, S. and Ibrahim, M. H. I. (2009) Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method. In: South East Asian Technical Universities Consortium(SEATUC) - 3rd SEATUC Symposium Proceeding, 25th - 26th February 2009, Johor Bahru, Malaysia.
institution Universiti Teknologi Malaysia
building UTM Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Teknologi Malaysia
content_source UTM Institutional Repository
url_provider http://eprints.utm.my/
language English
topic TJ Mechanical engineering and machinery
TS Manufactures
spellingShingle TJ Mechanical engineering and machinery
TS Manufactures
Jamaludin, K. R.
Muhamad, N.
Ab. Rahman, M. N.
M. Amin, S. Y.
Ahmad, S.
Ibrahim, M. H. I.
Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method
description Sintering parameters of the SS316L water atomised injection moulded compact has been optimized for its best sintered density. The L9 (34) Taguchi orthogonal array is used in the experiment while sintering temperature, sintering time, heating rate and coofing rate was selected as factors that influenced the sintered density. The sintering environment was in the vacuum and four replications were done for each trial. The analysis of variance shows that the confident level for the experiment was 99.5 % (a = 0.005) and all factors are highly significant at a =0.005 to the sintered density. The study concluded that the heating rate has the highest influence to the sintered density (41.29 %) followed by sintering temperature (31.60 %) , sintering time (11.13 %) and cooling rate (11.10%). The optimum sintered density obtained is 98.48 % of the theoretical density and the optimum parameter has been verified that the sintered density obtained is in a range of confident interval.
format Conference or Workshop Item
author Jamaludin, K. R.
Muhamad, N.
Ab. Rahman, M. N.
M. Amin, S. Y.
Ahmad, S.
Ibrahim, M. H. I.
author_facet Jamaludin, K. R.
Muhamad, N.
Ab. Rahman, M. N.
M. Amin, S. Y.
Ahmad, S.
Ibrahim, M. H. I.
author_sort Jamaludin, K. R.
title Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method
title_short Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method
title_full Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method
title_fullStr Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method
title_full_unstemmed Sintering parameter optimisation of the SS316L Metal Injection Molding (MIM) compacts for final density using taguchi method
title_sort sintering parameter optimisation of the ss316l metal injection molding (mim) compacts for final density using taguchi method
publishDate 2009
url http://eprints.utm.my/id/eprint/12620/1/KRJamaludin2008_SinteringParameterOptimisationoftheSS316LMetal.pdf
http://eprints.utm.my/id/eprint/12620/
_version_ 1643646000425861120