Prestress loss of post-tensioned clay diaphragm and fin brickwork
Unlike calcium silicate and concrete block masonry which undergo shrinkage with time, clay brickwork has been known to expand instead. Expansion of brick units in prestressed masonry will cause an increase in the prestressing force instead of prestress loss. However, not all clay brickwork expand wi...
Saved in:
Main Author: | |
---|---|
Format: | Article |
Language: | English |
Published: |
Faculty of Civil Engineering, Universiti Teknologi Malaysia
1994
|
Subjects: | |
Online Access: | http://eprints.utm.my/id/eprint/27859/1/SitiHamisabTapsir1994_PrestressLossofPostTensionedClay.pdf http://eprints.utm.my/id/eprint/27859/ http://www.civil.utm.my/content.php?id=387&cid=204&lang=1 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Teknologi Malaysia |
Language: | English |
id |
my.utm.27859 |
---|---|
record_format |
eprints |
spelling |
my.utm.278592012-08-10T03:39:24Z http://eprints.utm.my/id/eprint/27859/ Prestress loss of post-tensioned clay diaphragm and fin brickwork Tapsir, Siti Hamisab TA Engineering (General). Civil engineering (General) Unlike calcium silicate and concrete block masonry which undergo shrinkage with time, clay brickwork has been known to expand instead. Expansion of brick units in prestressed masonry will cause an increase in the prestressing force instead of prestress loss. However, not all clay brickwork expand with time; higher strength clay units tend to undergo shrinkage with time. The main objective of this paper is to present experimental data obtained for prestress loss in post-tensioned high strength clay diaphragm and fin brickwork. The main objective of this paper is to present experimental data obtained for prestress loss in posttensioned high strength clay diaphragm and fin brickwork. The brickwork were built from clmisB clay engineering brick with compressive strength of 103 MPa with designation (ii) mortar. The tests which involve monitoring prestress loss, creep and shrinkage of clay sections were carried out over a period of 120 days. Usiog the 120-day experimental data, the predicted long-term prestress loss is 20% Faculty of Civil Engineering, Universiti Teknologi Malaysia 1994 Article PeerReviewed application/pdf en http://eprints.utm.my/id/eprint/27859/1/SitiHamisabTapsir1994_PrestressLossofPostTensionedClay.pdf Tapsir, Siti Hamisab (1994) Prestress loss of post-tensioned clay diaphragm and fin brickwork. Jurnal Kejuruteraan Awam, 7 (2). pp. 12-18. ISSN 0128-0147 http://www.civil.utm.my/content.php?id=387&cid=204&lang=1 |
institution |
Universiti Teknologi Malaysia |
building |
UTM Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Teknologi Malaysia |
content_source |
UTM Institutional Repository |
url_provider |
http://eprints.utm.my/ |
language |
English |
topic |
TA Engineering (General). Civil engineering (General) |
spellingShingle |
TA Engineering (General). Civil engineering (General) Tapsir, Siti Hamisab Prestress loss of post-tensioned clay diaphragm and fin brickwork |
description |
Unlike calcium silicate and concrete block masonry which undergo shrinkage with time, clay brickwork has been known to expand instead. Expansion of brick units in prestressed masonry will cause an increase in the prestressing force instead of prestress loss. However, not all clay brickwork expand with time; higher strength clay units tend to undergo shrinkage with time. The main objective of this paper is to present experimental data obtained for prestress loss in post-tensioned high strength clay diaphragm and fin brickwork. The main objective of this paper is to present experimental data obtained for prestress loss in posttensioned high strength clay diaphragm and fin brickwork. The brickwork were built from clmisB clay engineering brick with compressive strength of 103 MPa with designation (ii) mortar. The tests which involve monitoring prestress loss, creep and shrinkage of clay sections were carried out over a period of 120 days. Usiog the 120-day experimental data, the predicted long-term prestress loss is 20% |
format |
Article |
author |
Tapsir, Siti Hamisab |
author_facet |
Tapsir, Siti Hamisab |
author_sort |
Tapsir, Siti Hamisab |
title |
Prestress loss of post-tensioned clay diaphragm and fin brickwork |
title_short |
Prestress loss of post-tensioned clay diaphragm and fin brickwork |
title_full |
Prestress loss of post-tensioned clay diaphragm and fin brickwork |
title_fullStr |
Prestress loss of post-tensioned clay diaphragm and fin brickwork |
title_full_unstemmed |
Prestress loss of post-tensioned clay diaphragm and fin brickwork |
title_sort |
prestress loss of post-tensioned clay diaphragm and fin brickwork |
publisher |
Faculty of Civil Engineering, Universiti Teknologi Malaysia |
publishDate |
1994 |
url |
http://eprints.utm.my/id/eprint/27859/1/SitiHamisabTapsir1994_PrestressLossofPostTensionedClay.pdf http://eprints.utm.my/id/eprint/27859/ http://www.civil.utm.my/content.php?id=387&cid=204&lang=1 |
_version_ |
1643647960389517312 |