Fabrication and characterization of polymer thermo-optic switch based on MMI coupler
The 2×2 polymer thermo-optic switch based on MMI coupler is realized. This device is fabricated using standard fabrication techniques such as coating, photolithography, and dry etching. A crosstalk level of -36.2 dB is achieved at cross and bar states. A power consumption of 1.85 mW is applied to ch...
Saved in:
Main Authors: | , , , , |
---|---|
Format: | Article |
Published: |
Elsevier B.V.
2011
|
Subjects: | |
Online Access: | http://eprints.utm.my/id/eprint/29679/ http://dx.doi.org/10.1016/j.optcom.2010.10.025 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Teknologi Malaysia |
Summary: | The 2×2 polymer thermo-optic switch based on MMI coupler is realized. This device is fabricated using standard fabrication techniques such as coating, photolithography, and dry etching. A crosstalk level of -36.2 dB is achieved at cross and bar states. A power consumption of 1.85 mW is applied to change the state of the switch from the cross to the bar state. A switching time of less than 0.7 ms is traced to change a state of the realized switch. |
---|