Synthesis and characterization of gold nanoparticles for mercury adsorption

This research was carried out to synthesize and characterize different sizes and shapes of gold (Au) nanoparticles in order to find the optimum synthesis parameters for maximum mercury adsorption. The different sizes and shapes of Au nanoparticles were prepared using microwave (MW) polyol method. By...

Full description

Saved in:
Bibliographic Details
Main Author: Mohamad, Mawarni Fazliana
Format: Thesis
Language:English
Published: 2012
Subjects:
Online Access:http://eprints.utm.my/id/eprint/81100/1/MawarniFazlianaMohamadMFPREE2012.pdf
http://eprints.utm.my/id/eprint/81100/
http://dms.library.utm.my:8080/vital/access/manager/Repository/vital:119071
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universiti Teknologi Malaysia
Language: English
id my.utm.81100
record_format eprints
spelling my.utm.811002019-07-24T03:09:42Z http://eprints.utm.my/id/eprint/81100/ Synthesis and characterization of gold nanoparticles for mercury adsorption Mohamad, Mawarni Fazliana TP Chemical technology This research was carried out to synthesize and characterize different sizes and shapes of gold (Au) nanoparticles in order to find the optimum synthesis parameters for maximum mercury adsorption. The different sizes and shapes of Au nanoparticles were prepared using microwave (MW) polyol method. By using different polyvinylpyrrolidone (PVP) concentrations (1.9-33.3 mM), different concentration of sodium chloride (NaCl) (10-30 mM) and different amount of [Au]1/[Au]0 molar ratio (1-9), different sizes and shapes of Au nanoparticles were obtained. The Au nanoparticles were characterized using ultra violet-visible (UVVis) absorption spectroscopy and transmission electron microscopy (TEM). The different sizes and various mixtures of spherical, triangular, cubic, hexagonal, octahedral, decahedral, icosahedral and one-dimension (1-D) particles were obtained using those methods. Mercury adsorption was determined based on different sizes and shapes of Au nanoparticles and measured using atomic absorption spectrophotometer (AAS). The optimum PVP concentration is 22.2 mM for 92 % spherical particles of a size in range less than 10 nm. It was found that, using 11.1 mM of PVP solution, the sizes and shapes can be further reduced in the presence of chloride ions. It was also found that, 20 mM of NaCl is sufficient to produce stable Au nanoparticles with most of the particles are spherical in which 97 % of particles diameter is less than 10 nm. The different of [Au]1/[Au]0 molar ratio led to the high yield of polygonal nanoparticles and the size is increase with increasing [Au]1/[Au]0 molar ratio. However, the optimum values of [Au]1/[Au]0 molar ratio cannot be determined because the sizes and shapes are irregular. High mercury adsorption was obtained for spherical nanoparticles (263.18 mg/g) with 99 % particles size less than 10 nm. The defect on spherical nanoparticles surface contributes to high mercury adsorption. In addition, smaller sizes of Au nanoparticles increase the total surface area available for mercury adsorption. It was found that the formation of sizes and shapes of Au nanoparticles was depend on parameters such as the concentration of PVP, NaCl, as well as [Au]1/[Au]0 molar ratio, and thus affects the mercury adsorption. 2012-05 Thesis NonPeerReviewed application/pdf en http://eprints.utm.my/id/eprint/81100/1/MawarniFazlianaMohamadMFPREE2012.pdf Mohamad, Mawarni Fazliana (2012) Synthesis and characterization of gold nanoparticles for mercury adsorption. Masters thesis, Universiti Teknologi Malaysia, Faculty of Petroleum and Renewable Energy Engineering. http://dms.library.utm.my:8080/vital/access/manager/Repository/vital:119071
institution Universiti Teknologi Malaysia
building UTM Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Teknologi Malaysia
content_source UTM Institutional Repository
url_provider http://eprints.utm.my/
language English
topic TP Chemical technology
spellingShingle TP Chemical technology
Mohamad, Mawarni Fazliana
Synthesis and characterization of gold nanoparticles for mercury adsorption
description This research was carried out to synthesize and characterize different sizes and shapes of gold (Au) nanoparticles in order to find the optimum synthesis parameters for maximum mercury adsorption. The different sizes and shapes of Au nanoparticles were prepared using microwave (MW) polyol method. By using different polyvinylpyrrolidone (PVP) concentrations (1.9-33.3 mM), different concentration of sodium chloride (NaCl) (10-30 mM) and different amount of [Au]1/[Au]0 molar ratio (1-9), different sizes and shapes of Au nanoparticles were obtained. The Au nanoparticles were characterized using ultra violet-visible (UVVis) absorption spectroscopy and transmission electron microscopy (TEM). The different sizes and various mixtures of spherical, triangular, cubic, hexagonal, octahedral, decahedral, icosahedral and one-dimension (1-D) particles were obtained using those methods. Mercury adsorption was determined based on different sizes and shapes of Au nanoparticles and measured using atomic absorption spectrophotometer (AAS). The optimum PVP concentration is 22.2 mM for 92 % spherical particles of a size in range less than 10 nm. It was found that, using 11.1 mM of PVP solution, the sizes and shapes can be further reduced in the presence of chloride ions. It was also found that, 20 mM of NaCl is sufficient to produce stable Au nanoparticles with most of the particles are spherical in which 97 % of particles diameter is less than 10 nm. The different of [Au]1/[Au]0 molar ratio led to the high yield of polygonal nanoparticles and the size is increase with increasing [Au]1/[Au]0 molar ratio. However, the optimum values of [Au]1/[Au]0 molar ratio cannot be determined because the sizes and shapes are irregular. High mercury adsorption was obtained for spherical nanoparticles (263.18 mg/g) with 99 % particles size less than 10 nm. The defect on spherical nanoparticles surface contributes to high mercury adsorption. In addition, smaller sizes of Au nanoparticles increase the total surface area available for mercury adsorption. It was found that the formation of sizes and shapes of Au nanoparticles was depend on parameters such as the concentration of PVP, NaCl, as well as [Au]1/[Au]0 molar ratio, and thus affects the mercury adsorption.
format Thesis
author Mohamad, Mawarni Fazliana
author_facet Mohamad, Mawarni Fazliana
author_sort Mohamad, Mawarni Fazliana
title Synthesis and characterization of gold nanoparticles for mercury adsorption
title_short Synthesis and characterization of gold nanoparticles for mercury adsorption
title_full Synthesis and characterization of gold nanoparticles for mercury adsorption
title_fullStr Synthesis and characterization of gold nanoparticles for mercury adsorption
title_full_unstemmed Synthesis and characterization of gold nanoparticles for mercury adsorption
title_sort synthesis and characterization of gold nanoparticles for mercury adsorption
publishDate 2012
url http://eprints.utm.my/id/eprint/81100/1/MawarniFazlianaMohamadMFPREE2012.pdf
http://eprints.utm.my/id/eprint/81100/
http://dms.library.utm.my:8080/vital/access/manager/Repository/vital:119071
_version_ 1643658610508562432