Fabrication and morphology charaterization of spin-coated nafion thin films
Nafion thin films {<2um) were fabricated using the spin coating technique. Substrate (silicon, silica and glass), concentration (5%, 10%, and 15% Nafion concentration), and spin coating angular velocity (1500rpm, 2000rpm, and 2500rpm) were chosen as the parameters. The deposition of the films ont...