B6O ceramic by in-situ reactive spark plasma sintering of a B2O3 and B powder mixture
A mixture of B2O3 and amorphous B with the mole ratio of 1:14 is shown to react and form B6O ceramic under in-situ spark plasma sintering (SPS) conditions. The optimum SPS temperature and time to obtain phase B6O are 1250°C and 30 min, respectively, and Rietveld refinement of the XRD patterns indica...
Saved in:
Main Authors: | Sakka, Yoshio, Badica, Petre, Vasylkiv, Oleg, Solodkyi, Levgen, Borodianska, Hanna, Zhao, Ting |
---|---|
Other Authors: | Temasek Laboratories |
Format: | Article |
Language: | English |
Published: |
2014
|
Subjects: | |
Online Access: | https://hdl.handle.net/10356/105277 http://hdl.handle.net/10220/20518 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Nanyang Technological University |
Language: | English |
Similar Items
-
Tough and dense boron carbide obtained by high-pressure (300 MPa) and low-temperature (1600°C) spark plasma sintering
by: Badica, Petre, et al.
Published: (2014) -
Grain boundary diffusion driven spark plasma sintering of nanocrystalline zirconia
by: Borodianska, Hanna, et al.
Published: (2013) -
Metal-ceramic/ceramic nanostructured layered composites for solid oxide fuel cells by spark plasma sintering
by: Bezdorozhev, Oleksii, et al.
Published: (2014) -
Spark plasma sintered Ni-YSZ/YSZ bi-layers for solid oxide fuel cell
by: Bezdorozhev, Oleksii, et al.
Published: (2014) -
Consolidation of B4C-TaB2 eutectic composites by spark plasma sintering
by: Demirskyi, Dmytro, et al.
Published: (2016)