Recycling bacteria for the synthesis of LiMPO4 (M = Fe, Mn) nanostructures for high-power lithium batteries

In this work, a novel waste-to-resource strategy to convert waste bacteria into a useful class of cathode materials, lithium metal phosphate (LiMPO4; M = Fe, Mn), is presented. Escherichia coli (E. coli) bacteria used for removing phosphorus contamination from wastewater are harvested and used as pr...

Full description

Saved in:
Bibliographic Details
Main Authors: Zhou, Yanping, Yang, Dan, Zeng, Yi, Zhou, Yan, Ng, Wun Jern, Yan, Qingyu, Fong, Eileen
Other Authors: School of Materials Science & Engineering
Format: Article
Language:English
Published: 2014
Subjects:
Online Access:https://hdl.handle.net/10356/105315
http://hdl.handle.net/10220/20470
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
Description
Summary:In this work, a novel waste-to-resource strategy to convert waste bacteria into a useful class of cathode materials, lithium metal phosphate (LiMPO4; M = Fe, Mn), is presented. Escherichia coli (E. coli) bacteria used for removing phosphorus contamination from wastewater are harvested and used as precursors for the synthesis of LiMPO4. After annealing, LiFePO4 and LiMnPO4 nanoparticles with dimensions around 20 nm are obtained. These particles are found to be enveloped in a carbon layer with a thickness around 3–5 nm, generated through the decomposition of the organic matter from the bacterial cell cytoplasm. The battery performance for the LiFePO4 is evaluated. A high discharge capacity of 140 mAh g−1 at 0.1 C with a flat plateau located at around 3.5 V is obtained. In addition, the synthesized particles display excellent stability and rate capabilities. Even under a high C rate of 10 C, a stable discharge capacity of 75.4 mAh g−1 can still be achieved.