Periodic FTO IOs/CdS NRs/CdSe clusters with superior light scattering ability for improved photoelectrochemical performance

Periodic fluorine-doped tin oxide inverse opals (FTO IOs) grafted with CdS nanorods (NRs) and CdSe clusters are reported for improved photoelectrochemical (PEC) performance. This hierarchical photoanode is fabricated by a combination of dip-coating, hydrothermal reaction, and chemical bath depositio...

Full description

Saved in:
Bibliographic Details
Main Authors: Wang, Zhiwei, Nguyen, Tam Duy, Yeo, Loo Pin, Tan, Chiew Kei, Gan, Lin, Tok, Alfred Iing Yoong
Other Authors: School of Materials Science and Engineering
Format: Article
Language:English
Published: 2022
Subjects:
Online Access:https://hdl.handle.net/10356/155261
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
Description
Summary:Periodic fluorine-doped tin oxide inverse opals (FTO IOs) grafted with CdS nanorods (NRs) and CdSe clusters are reported for improved photoelectrochemical (PEC) performance. This hierarchical photoanode is fabricated by a combination of dip-coating, hydrothermal reaction, and chemical bath deposition. The growth of 1D CdS NRs on the periodic walls of 3D FTO IOs forms a unique 3D/1D hierarchical structure, providing a sizeable specific surface area for the loading of CdSe clusters. Significantly, the periodic FTO IOs enable uniform light scattering while the abundant surrounded CdS NRs induce additional random light scattering, combining to give multiple light scattering within the complete hierarchical structure, significantly improving light-harvesting of CdS NRs and CdSe clusters. The high electron collection ability of FTO IOs and the CdS/CdSe heterojunction formation also contribute to the enhanced charge transport and separation. Due to the incorporation of these enhancement strategies in one hierarchical structure, FTO IOs/CdS NRs/CdSe clusters present an improved PEC performance. The photocurrent density of FTO IOs/CdS NRs/CdSe clusters at 1.23 V versus reversible hydrogen electrode reaches 9.2 mA cm-2 , which is 1.43 times greater than that of CdS NRs/CdSe clusters and 3.83 times of CdS NRs.