Air-tolerant reversible complexation mediated polymerization (RCMP) using aldehyde

An air-tolerant reversible complexation mediated polymerization (RCMP) technique, which can be carried out without prior deoxygenation, is developed. The system contains a monomer, an alkyl iodide initiating dormant species, air (oxygen), an aldehyde, N-hydroxyphthalimide (NHPI), and a base. Oxygen...

Full description

Saved in:
Bibliographic Details
Main Authors: Mao, Weijia, Tay, Xiu Ting, Sarkar, Jit, Wang, Chen-Gang, Goto, Atsushi
Other Authors: School of Physical and Mathematical Sciences
Format: Article
Language:English
Published: 2022
Subjects:
Online Access:https://hdl.handle.net/10356/156730
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
Description
Summary:An air-tolerant reversible complexation mediated polymerization (RCMP) technique, which can be carried out without prior deoxygenation, is developed. The system contains a monomer, an alkyl iodide initiating dormant species, air (oxygen), an aldehyde, N-hydroxyphthalimide (NHPI), and a base. Oxygen is consumed via the NHPI-catalyzed conversion of the aldehyde (RCHO) to a carboxylic acid (RCOOH). The generated RCOOH is further converted to a carboxylate anion (RCOO- ) by the base. The RCOO- generated in situ works as an RCMP catalyst; the polymerization proceeds with the monomer, alkyl iodide dormant species, and RCOO- catalyst. Thus, the system is not only air-tolerant but also does not require additional RCMP catalysts, which is a notable feature of this system. (NHPI is used as an oxidation catalyst for converting RCHO to RCOOH.) This technique is amenable to methyl methacrylate, butyl methacrylate, benzyl methacrylate, 2-hydroxyethyl methacrylate, and styrene, yielding polymers with relatively low-dispersity (Mw /Mn  = 1.20-1.49), where Mw and Mn are the weight- and number-average molecular weights, respectively.