Effects of modifier (Gd, Sc, La) addition on the stability of low Ni content catalyst for dry reforming of model biogas

Biogas consists of a larger part of methane and a smaller part of carbon dioxide. Reforming biogas is highly desirable due to the direct conversion of the two components, yet not possible due to the current state of catalyst development. For such dry reforming of methane-rich gases (CH4/CO2 = 2) we...

Full description

Saved in:
Bibliographic Details
Main Authors: Quan Luu Manh Ha, Atia, Hanan, Kreyenschulte, Carsten, Lund, Henrik, Bartling, Stephan, Lisak, Grzegorz, Wohlrab, Sebastian, Armbruster, Udo
Other Authors: School of Civil and Environmental Engineering
Format: Article
Language:English
Published: 2022
Subjects:
Online Access:https://hdl.handle.net/10356/159575
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
Description
Summary:Biogas consists of a larger part of methane and a smaller part of carbon dioxide. Reforming biogas is highly desirable due to the direct conversion of the two components, yet not possible due to the current state of catalyst development. For such dry reforming of methane-rich gases (CH4/CO2 = 2) we now present catalysts with low Ni loading (2.5 wt%) modified with Gd, Sc, or La. The best catalyst reaches 49% CH4 conversion and 95% CO2 conversion at 750 °C. The La-modification only shows limited influence on coking and protection against catalyst deactivation although this catalyst exposed highest basicity. On the other side, Sc- and especially Gd-modified catalysts exposed stronger metal-support interaction and thus enhanced stabilization of fine Ni particles during the reaction, which is critical to preserve high performance in CH4-rich DRM. This suppressed carbon deposition and the growth of structured carbon as evidenced by STEM images and TPO of spent catalysts. In this way, exceptionally high specific H2 productivity (94 l/(gcat·h)) compared to literature was obtained on Gd-modified catalyst, and, most noteworthy, after extending the time on stream from 8 to 100 h the amount of deposited coke increased only from 3 to 4 wt%.