Fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions

In order to understand the fatigue growth behaviors of tubular joints, large-scale tubular joint fatigue tests had been performed for a number of decades. But most of them were tested under basic loading, i.e. axial load (AX), in-plane-bending (IPB) and out-of-plane (OPB). In the current test progra...

Full description

Saved in:
Bibliographic Details
Main Author: Lie, Seng Tjhen.
Other Authors: School of Civil and Environmental Engineering
Format: Research Report
Language:English
Published: 2009
Subjects:
Online Access:http://hdl.handle.net/10356/17238
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
id sg-ntu-dr.10356-17238
record_format dspace
spelling sg-ntu-dr.10356-172382023-03-03T16:44:25Z Fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions Lie, Seng Tjhen. School of Civil and Environmental Engineering DRNTU::Engineering::Civil engineering::Structures and design In order to understand the fatigue growth behaviors of tubular joints, large-scale tubular joint fatigue tests had been performed for a number of decades. But most of them were tested under basic loading, i.e. axial load (AX), in-plane-bending (IPB) and out-of-plane (OPB). In the current test program, full-scale circular hollow sections (CHS) and rectangular hollow sections (RHS) tubular joints were tested under the basic and combined loading so as to understand their fatigue crack growth behaviors as well as their fatigue strengths. The tests in this research project include experimental stress analyses under basic and combined loading and fatigue tests under basic and combined loading. The static tests were carried out first to determine the stress concentration factors (SCFs) of the joints, and the peak hot spot stress (HSS) locations where the cracks may initiate. The SCF results are also used to compare with some of the well-established existing SCF equations. In the past decades, many tests on tubular joints had been performed (van Delft et al., 1986; Ritchie et al., 1989; Myers, 1998 etc.), but the 3D crack shapes formed during propagation were scarcely captured in these fatigue tests. Therefore, it is difficult to model the accurate crack surface in finite element models which may produce inaccurate stress intensity factors solution. In order to validate the stress intensity factors along the crack front of the tubular joints for the next phase of the research project, fatigue tests were carried out whereby the 3D crack propagation and profiles were monitored using the Alternating Current Potential Drop (ACPD) technique, and hence the fatigue strengths of these specimens. RG 04/01 2009-06-02T01:42:39Z 2009-06-02T01:42:39Z 2007 2007 Research Report http://hdl.handle.net/10356/17238 en 147 p. application/pdf
institution Nanyang Technological University
building NTU Library
continent Asia
country Singapore
Singapore
content_provider NTU Library
collection DR-NTU
language English
topic DRNTU::Engineering::Civil engineering::Structures and design
spellingShingle DRNTU::Engineering::Civil engineering::Structures and design
Lie, Seng Tjhen.
Fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions
description In order to understand the fatigue growth behaviors of tubular joints, large-scale tubular joint fatigue tests had been performed for a number of decades. But most of them were tested under basic loading, i.e. axial load (AX), in-plane-bending (IPB) and out-of-plane (OPB). In the current test program, full-scale circular hollow sections (CHS) and rectangular hollow sections (RHS) tubular joints were tested under the basic and combined loading so as to understand their fatigue crack growth behaviors as well as their fatigue strengths. The tests in this research project include experimental stress analyses under basic and combined loading and fatigue tests under basic and combined loading. The static tests were carried out first to determine the stress concentration factors (SCFs) of the joints, and the peak hot spot stress (HSS) locations where the cracks may initiate. The SCF results are also used to compare with some of the well-established existing SCF equations. In the past decades, many tests on tubular joints had been performed (van Delft et al., 1986; Ritchie et al., 1989; Myers, 1998 etc.), but the 3D crack shapes formed during propagation were scarcely captured in these fatigue tests. Therefore, it is difficult to model the accurate crack surface in finite element models which may produce inaccurate stress intensity factors solution. In order to validate the stress intensity factors along the crack front of the tubular joints for the next phase of the research project, fatigue tests were carried out whereby the 3D crack propagation and profiles were monitored using the Alternating Current Potential Drop (ACPD) technique, and hence the fatigue strengths of these specimens.
author2 School of Civil and Environmental Engineering
author_facet School of Civil and Environmental Engineering
Lie, Seng Tjhen.
format Research Report
author Lie, Seng Tjhen.
author_sort Lie, Seng Tjhen.
title Fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions
title_short Fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions
title_full Fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions
title_fullStr Fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions
title_full_unstemmed Fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions
title_sort fatigue strength of circular and rectangular hollow sections subjected to complex loading conditions
publishDate 2009
url http://hdl.handle.net/10356/17238
_version_ 1759853991546585088