Tensile properties of styrene-ethylene-butadiene-styrene toughened and glass fiber reinforced polyethylene
Polyethylene composites reinforced with glass fibers and elastomer-toughened with styrene-ethylene-butadiene-styrene were prepared using extrusion and then compression molded to form tensile bars conforming to the ASTM D-638 testing standards. Varying amounts of glass fibers and SEBS elastomers were...
Saved in:
Main Author: | Wong, Ngiap Han. |
---|---|
Other Authors: | Tan Lay Poh |
Format: | Final Year Project |
Language: | English |
Published: |
2010
|
Subjects: | |
Online Access: | http://hdl.handle.net/10356/38599 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Nanyang Technological University |
Language: | English |
Similar Items
-
Development of polyethylene's properties by utilizing glass fiber and styrene-ethylene-butylene-styrene block copolymer (SEBS2)
by: Agus, Marlene
Published: (2010) -
Comparison on properties of acrylonitrile styrene butadiene rubber (nsbr) and styrene butadiene rubber (sbr) /nitrile rubber (NBR) blends
by: Yotwadee Chokanandsombat, et al.
Published: (2018) -
Thermal, mechanical and tribological properties of polycarbonate/acrylonitrile-butadiene-styrene blends
by: Khun, Nay Win., et al.
Published: (2013) -
Compatibilization of high impact polystyrene/high density polyethylene blends by styrene/ethylene-butylene/styrene block copolymer
by: Asira Chirawithayaboon
Published: (2009) -
Polymer electrolytes based on acrylonitrile-butadiene-styrene copolymer
by: Hou, X., et al.
Published: (2014)