Dielectric elastomer generator
In this project, the performance of the graphite and silver as electrodes on Dielectric Elastomer Generator (DEG) were studied. With various strains applied on the dielectric layer as well as the initial voltages applied on the electrodes, the samples were tested and measured. These results...
Saved in:
Main Author: | |
---|---|
Other Authors: | |
Format: | Final Year Project |
Language: | English |
Published: |
2013
|
Subjects: | |
Online Access: | http://hdl.handle.net/10356/54180 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Nanyang Technological University |
Language: | English |
Summary: | In this project, the performance of the graphite and silver as electrodes on Dielectric
Elastomer Generator (DEG) were studied. With various strains applied on the dielectric layer
as well as the initial voltages applied on the electrodes, the samples were tested and measured.
These results were useful in the analysis for the efficiency of energy harvesting in future.
The fabrication process and the difficulties encountered were elaborated prior to the
commencement of experimental exploration. The working principle and theory for DEG was
covered in literature review which had been used to analyze the experimental data obtained.
There were some findings and verifications through the study.
There were some findings in this project. The efficiency was dependent on the initial charging
voltages and the pre-strains. From the results, the initial primed voltage applied would affect on
the energy generated. The higher initial voltage, the better average energy conversion
performance but up to breakdown limit of individual electrode materials. The best performance
of the voltage generation for both of graphite (340% increment) and silver electrodes (130%
increment) was at 0.5 kV prime voltage. Initial voltage of 1KV looked more representative for
its stability for graphite electrode while the initial voltage of 1.5KV more favourable for silver
electrode. But less effective voltage generated was observed with higher pre-strain.
The voltage and the capacitance were inversely proportional to each other provided the charge
was constant. The change in area under different pre-strain will be measured and the changes
in thickness of dielectric layer were used to calculate the theoretical capacitances. With that,
the estimation of voltage generation could be achieved for given charges.
To quantify the charge loss from DEG was another issue which to be addressed. The
conductivity or resistance of the different electrodes would cause some loss of charge from
DEG. The conductivity of the electrodes and the capacitance of the dielectric layer were also
measured. The results could be used to compare the theoretical and experimental values and
determined how accurate of the experiment could be. In additional, there were some other
factors affecting the efficiency of DEG. Upon accomplishing this project, the author realized
that there were still plenty rooms for future researches and improvement in this field of study. |
---|