Spark plasma sintering of boron carbide composite for defense application

Boron carbide is a very attractive material for use in armour applications because of the high hardness and the relatively low density it possesses. However, the difficulties in consolidating the material present a huge hurdle to overcome. Using conventional consolidation techniques, high sintering...

Full description

Saved in:
Bibliographic Details
Main Author: Png, Wee Chun
Other Authors: Alfred Tok Iing Yoong
Format: Final Year Project
Language:English
Published: 2014
Subjects:
Online Access:http://hdl.handle.net/10356/55792
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
id sg-ntu-dr.10356-55792
record_format dspace
spelling sg-ntu-dr.10356-557922023-03-04T15:41:59Z Spark plasma sintering of boron carbide composite for defense application Png, Wee Chun Alfred Tok Iing Yoong School of Materials Science and Engineering DRNTU::Engineering::Materials::Defence materials Boron carbide is a very attractive material for use in armour applications because of the high hardness and the relatively low density it possesses. However, the difficulties in consolidating the material present a huge hurdle to overcome. Using conventional consolidation techniques, high sintering temperature and long sintering time are needed to achieve a near full-densification. But, by using spark plasma sintering (SPS), the sintering temperature and time can be greatly reduced. The ballistic performance of boron carbide in armour application has also been hard to establish, due to the many variables involved, such as projectile velocity, types of threat, geometry of the ceramic, etc. The Depth of Penetration (DOP) test was found to be quite satisfactory for evaluating the ballistic performance of boron carbide. In this study two boron carbide powder of different grain size were sintered at a temperature of 1850 ○C using the SPS technique. The sintered boron carbide tiles were then evaluated for ballistic performance against a tungsten long-rod penetrator, using the standard DOP test method. It was found that the mass efficiency of the tile increases with tile thickness at a projectile velocity of 1,000 m/s. At a higher projectile velocity of 1,400 m/s, the mass efficiency of the tile decreases with increasing tile thickness. The mass efficiency of the tiles was also found to be increasing when the projectile velocity increases from 1,000 to 1,400 m/s. It was found that the ballistic efficiency of the tile decreases with wider grain size distribution. It was also determined that the ballistic performance of the boron carbide tile which had a layered arrangement in armour design showed a marked improvement over the conventional homogeneous boron carbide tile. Bachelor of Engineering (Materials Engineering) 2014-03-31T06:11:17Z 2014-03-31T06:11:17Z 2014 2014 Final Year Project (FYP) http://hdl.handle.net/10356/55792 en Nanyang Technological University 45 p. application/pdf
institution Nanyang Technological University
building NTU Library
continent Asia
country Singapore
Singapore
content_provider NTU Library
collection DR-NTU
language English
topic DRNTU::Engineering::Materials::Defence materials
spellingShingle DRNTU::Engineering::Materials::Defence materials
Png, Wee Chun
Spark plasma sintering of boron carbide composite for defense application
description Boron carbide is a very attractive material for use in armour applications because of the high hardness and the relatively low density it possesses. However, the difficulties in consolidating the material present a huge hurdle to overcome. Using conventional consolidation techniques, high sintering temperature and long sintering time are needed to achieve a near full-densification. But, by using spark plasma sintering (SPS), the sintering temperature and time can be greatly reduced. The ballistic performance of boron carbide in armour application has also been hard to establish, due to the many variables involved, such as projectile velocity, types of threat, geometry of the ceramic, etc. The Depth of Penetration (DOP) test was found to be quite satisfactory for evaluating the ballistic performance of boron carbide. In this study two boron carbide powder of different grain size were sintered at a temperature of 1850 ○C using the SPS technique. The sintered boron carbide tiles were then evaluated for ballistic performance against a tungsten long-rod penetrator, using the standard DOP test method. It was found that the mass efficiency of the tile increases with tile thickness at a projectile velocity of 1,000 m/s. At a higher projectile velocity of 1,400 m/s, the mass efficiency of the tile decreases with increasing tile thickness. The mass efficiency of the tiles was also found to be increasing when the projectile velocity increases from 1,000 to 1,400 m/s. It was found that the ballistic efficiency of the tile decreases with wider grain size distribution. It was also determined that the ballistic performance of the boron carbide tile which had a layered arrangement in armour design showed a marked improvement over the conventional homogeneous boron carbide tile.
author2 Alfred Tok Iing Yoong
author_facet Alfred Tok Iing Yoong
Png, Wee Chun
format Final Year Project
author Png, Wee Chun
author_sort Png, Wee Chun
title Spark plasma sintering of boron carbide composite for defense application
title_short Spark plasma sintering of boron carbide composite for defense application
title_full Spark plasma sintering of boron carbide composite for defense application
title_fullStr Spark plasma sintering of boron carbide composite for defense application
title_full_unstemmed Spark plasma sintering of boron carbide composite for defense application