Fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by selective laser melting (3D printing)
Manufacturing technology has made significant progress over the years and additive manufacturing technology, specifically selective laser melting (SLM), is becoming increasingly popular with many industries. In the aviation industry, Ti-6Al-4V titanium alloy is one of the most widely used material d...
Saved in:
Main Author: | |
---|---|
Other Authors: | |
Format: | Final Year Project |
Language: | English |
Published: |
2016
|
Subjects: | |
Online Access: | http://hdl.handle.net/10356/68367 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Nanyang Technological University |
Language: | English |
id |
sg-ntu-dr.10356-68367 |
---|---|
record_format |
dspace |
spelling |
sg-ntu-dr.10356-683672023-03-04T19:09:14Z Fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by selective laser melting (3D printing) Tan, Chng Kiat Li Peifeng School of Mechanical and Aerospace Engineering DRNTU::Engineering::Aeronautical engineering::Materials of construction Manufacturing technology has made significant progress over the years and additive manufacturing technology, specifically selective laser melting (SLM), is becoming increasingly popular with many industries. In the aviation industry, Ti-6Al-4V titanium alloy is one of the most widely used material due to its excellent mechanical properties. Although SLM optimizes the usage of material and has the ability to produce parts with geometrical flexibility, the inherent process-related defects such as porosities and voids have resulted in mechanical inferiorities. Therefore, the project aims to evaluate the fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by SLM. As-built SLM Ti-6Al-4V with circular cross-sections were subjected to constant amplitude uniaxial fully reversed fatigue loading and fractographic analyses were conducted using a scanning electron microscope. In general, the SLM Ti-6Al-4V specimens demonstrated considerably lower fatigue performance as compared to those from reference literatures. This is mainly attributed to the SLM defects as fatigue cracks were observed to be initiated at voids and unfused regions. The fracture surfaces of the high cycle specimens were characterized by crack initiation, propagation and final rupture and an apparent endurance limit was encountered. In contrast, the low cycle specimens displayed no features of a fatigue failure. Future projects can incorporate specimens with different build orientations so that the effects of different build orientations on the fatigue behaviour can be studied and compared. Bachelor of Engineering (Aerospace Engineering) 2016-05-25T07:51:42Z 2016-05-25T07:51:42Z 2016 Final Year Project (FYP) http://hdl.handle.net/10356/68367 en Nanyang Technological University 107 p. application/pdf |
institution |
Nanyang Technological University |
building |
NTU Library |
continent |
Asia |
country |
Singapore Singapore |
content_provider |
NTU Library |
collection |
DR-NTU |
language |
English |
topic |
DRNTU::Engineering::Aeronautical engineering::Materials of construction |
spellingShingle |
DRNTU::Engineering::Aeronautical engineering::Materials of construction Tan, Chng Kiat Fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by selective laser melting (3D printing) |
description |
Manufacturing technology has made significant progress over the years and additive manufacturing technology, specifically selective laser melting (SLM), is becoming increasingly popular with many industries. In the aviation industry, Ti-6Al-4V titanium alloy is one of the most widely used material due to its excellent mechanical properties. Although SLM optimizes the usage of material and has the ability to produce parts with geometrical flexibility, the inherent process-related defects such as porosities and voids have resulted in mechanical inferiorities. Therefore, the project aims to evaluate the fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by SLM. As-built SLM Ti-6Al-4V with circular cross-sections were subjected to constant amplitude uniaxial fully reversed fatigue loading and fractographic analyses were conducted using a scanning electron microscope. In general, the SLM Ti-6Al-4V specimens demonstrated considerably lower fatigue performance as compared to those from reference literatures. This is mainly attributed to the SLM defects as fatigue cracks were observed to be initiated at voids and unfused regions. The fracture surfaces of the high cycle specimens were characterized by crack initiation, propagation and final rupture and an apparent endurance limit was encountered. In contrast, the low cycle specimens displayed no features of a fatigue failure. Future projects can incorporate specimens with different build orientations so that the effects of different build orientations on the fatigue behaviour can be studied and compared. |
author2 |
Li Peifeng |
author_facet |
Li Peifeng Tan, Chng Kiat |
format |
Final Year Project |
author |
Tan, Chng Kiat |
author_sort |
Tan, Chng Kiat |
title |
Fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by selective laser melting (3D printing) |
title_short |
Fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by selective laser melting (3D printing) |
title_full |
Fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by selective laser melting (3D printing) |
title_fullStr |
Fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by selective laser melting (3D printing) |
title_full_unstemmed |
Fatigue behaviour of Ti-6Al-4V titanium alloy fabricated by selective laser melting (3D printing) |
title_sort |
fatigue behaviour of ti-6al-4v titanium alloy fabricated by selective laser melting (3d printing) |
publishDate |
2016 |
url |
http://hdl.handle.net/10356/68367 |
_version_ |
1759855600561291264 |