Spark-plasma-sintering (SPS) of nanostructured and submicron titanium oxide powders
Spark-plasma-sintering (SPS) consolidation of submicron and nanostructured titanium oxide (TiO2) powders was performed between 800 and 1000 °C for 1 min. The results were compared with conventional sintering using electrical resistant furnace that was performed between 600 and 1000 °C for 120 min. T...