The extended growth of graphene oxide flakes using ethanol CVD

We report the extended growth of Graphene Oxide (GO) flakes using atmospheric pressure ethanol Chemical Vapor Deposition (CVD). GO was used to catalyze the deposition of carbon on a substrate in the ethanol CVD with Ar and H2 as carrier gases. Raman, SEM, XPS and AFM characterized the growth to be a...

Full description

Saved in:
Bibliographic Details
Main Authors: Huang, Jingfeng, Larisika, Melanie, Fam, Derrick Wen Hui, He, Qiyuan, Nimmo, Myra A., Nowak, Christoph, Tok, Alfred Iing Yoong
Other Authors: School of Materials Science & Engineering
Format: Article
Language:English
Published: 2013
Subjects:
Online Access:https://hdl.handle.net/10356/96949
http://hdl.handle.net/10220/9948
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
Description
Summary:We report the extended growth of Graphene Oxide (GO) flakes using atmospheric pressure ethanol Chemical Vapor Deposition (CVD). GO was used to catalyze the deposition of carbon on a substrate in the ethanol CVD with Ar and H2 as carrier gases. Raman, SEM, XPS and AFM characterized the growth to be a reduced GO (RGO) of <5 layers. This newly grown RGO possesses lower defect density with larger and increased distribution of sp2 domains than chemically reduced RGO. Furthermore this method without optimization reduces the relative standard deviation of electrical conductivity between chips, from 80.5% to 16.5%, enabling RGO to be used in practical electronic devices.