Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics
10.1016/j.cscm.2021.e00775
Saved in:
Main Authors: | , , , , , |
---|---|
Other Authors: | |
Format: | Article |
Published: |
Elsevier Ltd
2022
|
Subjects: | |
Online Access: | https://scholarbank.nus.edu.sg/handle/10635/233534 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | National University of Singapore |
id |
sg-nus-scholar.10635-233534 |
---|---|
record_format |
dspace |
spelling |
sg-nus-scholar.10635-2335342024-03-26T04:01:55Z Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics Hamzah, Hussein K. Huseien, Ghasan Fahim Asaad, Mohammad Ali Georgescu, Dan Paul Ghoshal, S. K. Alrshoudi, Fahed BUILDING Alkali-activated mortars Bottle glass wastes Drying shrinkage Nanoparticles Slag Sulphuric acid resistance 10.1016/j.cscm.2021.e00775 Case Studies in Construction Materials 15 e00775 2022-10-26T09:00:54Z 2022-10-26T09:00:54Z 2021-12-01 Article Hamzah, Hussein K., Huseien, Ghasan Fahim, Asaad, Mohammad Ali, Georgescu, Dan Paul, Ghoshal, S. K., Alrshoudi, Fahed (2021-12-01). Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics. Case Studies in Construction Materials 15 : e00775. ScholarBank@NUS Repository. https://doi.org/10.1016/j.cscm.2021.e00775 2214-5095 https://scholarbank.nus.edu.sg/handle/10635/233534 Attribution-NonCommercial-NoDerivatives 4.0 International https://creativecommons.org/licenses/by-nc-nd/4.0/ Elsevier Ltd Scopus OA2021 |
institution |
National University of Singapore |
building |
NUS Library |
continent |
Asia |
country |
Singapore Singapore |
content_provider |
NUS Library |
collection |
ScholarBank@NUS |
topic |
Alkali-activated mortars Bottle glass wastes Drying shrinkage Nanoparticles Slag Sulphuric acid resistance |
spellingShingle |
Alkali-activated mortars Bottle glass wastes Drying shrinkage Nanoparticles Slag Sulphuric acid resistance Hamzah, Hussein K. Huseien, Ghasan Fahim Asaad, Mohammad Ali Georgescu, Dan Paul Ghoshal, S. K. Alrshoudi, Fahed Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics |
description |
10.1016/j.cscm.2021.e00775 |
author2 |
BUILDING |
author_facet |
BUILDING Hamzah, Hussein K. Huseien, Ghasan Fahim Asaad, Mohammad Ali Georgescu, Dan Paul Ghoshal, S. K. Alrshoudi, Fahed |
format |
Article |
author |
Hamzah, Hussein K. Huseien, Ghasan Fahim Asaad, Mohammad Ali Georgescu, Dan Paul Ghoshal, S. K. Alrshoudi, Fahed |
author_sort |
Hamzah, Hussein K. |
title |
Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics |
title_short |
Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics |
title_full |
Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics |
title_fullStr |
Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics |
title_full_unstemmed |
Effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: Durability characteristics |
title_sort |
effect of waste glass bottles-derived nanopowder as slag replacement on mortars with alkali activation: durability characteristics |
publisher |
Elsevier Ltd |
publishDate |
2022 |
url |
https://scholarbank.nus.edu.sg/handle/10635/233534 |
_version_ |
1795301913204359168 |