Study of strontium ferrites substituted by lanthanum on the structural and magnetic properties

M-type strontium ferrites, Sr 0.8La 0.2Fe 12O 19 have been synthesized by conventional ceramic process. The effects of lanthanum addition and sintering temperature on microstructures and magnetic properties of SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 samples were investigated. Microstructural analysis...

Full description

Saved in:
Bibliographic Details
Main Authors: Onreabroy,W., Papato,K., Rujijanagul,G., Pengpat,K., Tunkasiri,T.
Format: Conference or Workshop Item
Published: Elsevier Limited 2015
Subjects:
Online Access:http://www.scopus.com/inward/record.url?partnerID=HzOxMe3b&scp=84655162128&origin=inward
http://cmuir.cmu.ac.th/handle/6653943832/38607
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
id th-cmuir.6653943832-38607
record_format dspace
spelling th-cmuir.6653943832-386072015-06-16T07:53:34Z Study of strontium ferrites substituted by lanthanum on the structural and magnetic properties Onreabroy,W. Papato,K. Rujijanagul,G. Pengpat,K. Tunkasiri,T. Surfaces, Coatings and Films Materials Chemistry Electronic, Optical and Magnetic Materials Ceramics and Composites Process Chemistry and Technology M-type strontium ferrites, Sr 0.8La 0.2Fe 12O 19 have been synthesized by conventional ceramic process. The effects of lanthanum addition and sintering temperature on microstructures and magnetic properties of SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 samples were investigated. Microstructural analysis of the SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 specimens, sintered at different temperatures revealed that average grain sizes of SrFe 12O 19 ferrites were larger than that of Sr 0.8La 0.2Fe 12O 19 ferrite and increased with increasing sintering temperature. The X-ray diffraction (XRD) results confirmed the strontium hexagonal ferrite phase of SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 compounds. A maximum coercivity value of 4850 Oe and maximum saturation magnetization value of 102 emu/g were obtained for the SrFe 12O 19 ferrite sintered at 1150°C and for the SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 ferrites sintered at 1300°C, respectively. The remanence (Mr) of Sr 0.8La 0.2Fe 12O 19 sample sintered at 1200°C possesses the maximum value of 60 emu/g. © 2011 Elsevier Ltd and Techna Group S.r.l. 2015-06-16T07:53:34Z 2015-06-16T07:53:34Z 2012-01-01 Conference Paper 02728842 2-s2.0-84655162128 10.1016/j.ceramint.2011.05.023 http://www.scopus.com/inward/record.url?partnerID=HzOxMe3b&scp=84655162128&origin=inward http://cmuir.cmu.ac.th/handle/6653943832/38607 Elsevier Limited
institution Chiang Mai University
building Chiang Mai University Library
country Thailand
collection CMU Intellectual Repository
topic Surfaces, Coatings and Films
Materials Chemistry
Electronic, Optical and Magnetic Materials
Ceramics and Composites
Process Chemistry and Technology
spellingShingle Surfaces, Coatings and Films
Materials Chemistry
Electronic, Optical and Magnetic Materials
Ceramics and Composites
Process Chemistry and Technology
Onreabroy,W.
Papato,K.
Rujijanagul,G.
Pengpat,K.
Tunkasiri,T.
Study of strontium ferrites substituted by lanthanum on the structural and magnetic properties
description M-type strontium ferrites, Sr 0.8La 0.2Fe 12O 19 have been synthesized by conventional ceramic process. The effects of lanthanum addition and sintering temperature on microstructures and magnetic properties of SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 samples were investigated. Microstructural analysis of the SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 specimens, sintered at different temperatures revealed that average grain sizes of SrFe 12O 19 ferrites were larger than that of Sr 0.8La 0.2Fe 12O 19 ferrite and increased with increasing sintering temperature. The X-ray diffraction (XRD) results confirmed the strontium hexagonal ferrite phase of SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 compounds. A maximum coercivity value of 4850 Oe and maximum saturation magnetization value of 102 emu/g were obtained for the SrFe 12O 19 ferrite sintered at 1150°C and for the SrFe 12O 19 and Sr 0.8La 0.2Fe 12O 19 ferrites sintered at 1300°C, respectively. The remanence (Mr) of Sr 0.8La 0.2Fe 12O 19 sample sintered at 1200°C possesses the maximum value of 60 emu/g. © 2011 Elsevier Ltd and Techna Group S.r.l.
format Conference or Workshop Item
author Onreabroy,W.
Papato,K.
Rujijanagul,G.
Pengpat,K.
Tunkasiri,T.
author_facet Onreabroy,W.
Papato,K.
Rujijanagul,G.
Pengpat,K.
Tunkasiri,T.
author_sort Onreabroy,W.
title Study of strontium ferrites substituted by lanthanum on the structural and magnetic properties
title_short Study of strontium ferrites substituted by lanthanum on the structural and magnetic properties
title_full Study of strontium ferrites substituted by lanthanum on the structural and magnetic properties
title_fullStr Study of strontium ferrites substituted by lanthanum on the structural and magnetic properties
title_full_unstemmed Study of strontium ferrites substituted by lanthanum on the structural and magnetic properties
title_sort study of strontium ferrites substituted by lanthanum on the structural and magnetic properties
publisher Elsevier Limited
publishDate 2015
url http://www.scopus.com/inward/record.url?partnerID=HzOxMe3b&scp=84655162128&origin=inward
http://cmuir.cmu.ac.th/handle/6653943832/38607
_version_ 1681421504292585472