Phase formation, dielectric and ferroelectric properties of Mn, Al Doped BCZT ceramics by molten salt method
Lead-free Ba(1-x)CaxZr0.1Ti 0.9O3 (x = 0.15) ceramics doped with 0.00-0.20 mol% MnO2 and Al2O3 were prepared by the molten salt method. The powder was ball-milled for 24 h and then calcined at 1000°C for 4 h and sintered at 1300°C for 2 h. The phase formation and dielectric properties of the ceramic...