Design of boiler welding for improvement of lifetime and cost control
© 2016 by the authors; licensee MDPI, Basel, Switzerland. Fe-2.25Cr-1Mo a widely used material for headers and steam tubes of boilers. Welding of steam tube to header is required for production of boiler. Heat affected zone of the weld can have poor mechanical properties and poor corrosion behavior...